LITHIUM GARNET AND METHODS OF MAKING THE SAME
Methods of making lithium garnet include combining a lithium source, a lanthanum source, a zirconium source, an optional dopant, and an optional lithium garnet seed crystal to form a precursor mixture. Methods include mixing the precursor mixture with a solvent to form a slurry. Methods include drying the slurry to form a solid precursor. Methods include calcining the solid precursor at a calcining temperature from about 900°C to about 1200°C for a period of time from about 2 minutes to about 40 minutes to form the lithium garnet. The lithium garnet can be formed into sintered sheets for use, for example, as electrodes or solid-state electrolytes.
Des procédés de fabrication de grenat de lithium comprennent la combinaison d'une source de lithium, d'une source de lanthane, d'une source de zirconium, d'un dopant facultatif et d'un germe de grenat de lithium facultatif pour former un mélange précurseur. Les procédés comprennent le mélange du mélange précurseur avec un solvant pour former une suspension. Les procédés comprennent le séchage de la suspension pour former un précurseur solide. Les procédés comprennent également la calcination du précurseur solide à une température de calcination d'environ 900 °C à environ 1200 °C pendant une période de temps d'environ 2 minutes à environ 40 minutes pour former le grenat de lithium. Le grenat de lithium peut être formé en feuilles frittées pour l'utilisation, par exemple, en tant qu'électrodes ou électrolytes à l'état solide.
LITHIUM GARNET AND METHODS OF MAKING THE SAME
Methods of making lithium garnet include combining a lithium source, a lanthanum source, a zirconium source, an optional dopant, and an optional lithium garnet seed crystal to form a precursor mixture. Methods include mixing the precursor mixture with a solvent to form a slurry. Methods include drying the slurry to form a solid precursor. Methods include calcining the solid precursor at a calcining temperature from about 900°C to about 1200°C for a period of time from about 2 minutes to about 40 minutes to form the lithium garnet. The lithium garnet can be formed into sintered sheets for use, for example, as electrodes or solid-state electrolytes.
Des procédés de fabrication de grenat de lithium comprennent la combinaison d'une source de lithium, d'une source de lanthane, d'une source de zirconium, d'un dopant facultatif et d'un germe de grenat de lithium facultatif pour former un mélange précurseur. Les procédés comprennent le mélange du mélange précurseur avec un solvant pour former une suspension. Les procédés comprennent le séchage de la suspension pour former un précurseur solide. Les procédés comprennent également la calcination du précurseur solide à une température de calcination d'environ 900 °C à environ 1200 °C pendant une période de temps d'environ 2 minutes à environ 40 minutes pour former le grenat de lithium. Le grenat de lithium peut être formé en feuilles frittées pour l'utilisation, par exemple, en tant qu'électrodes ou électrolytes à l'état solide.
LITHIUM GARNET AND METHODS OF MAKING THE SAME
GRENAT DE LITHIUM ET SES PROCÉDÉS DE FABRICATION
CONWAY BETHANY ROSE (author) / TEPESCH PATRICK DAVID (author) / VILENO ELIZABETH MARIE (author)
2024-04-25
Patent
Electronic Resource
English
European Patent Office | 2024
|European Patent Office | 2018
|European Patent Office | 2019
|European Patent Office | 2025
|European Patent Office | 2024
|