METHOD FOR PREPARING EARLY-STRENGTH LIQUID ACCELERATOR FREE OF ALKALI, CHLORINE, AND FLUORINE
The present invention provides a method for preparing an early-strength liquid accelerator free of alkali, chlorine, and fluorine. In percentage by mass and on the basis of the sum of the usage amounts of aluminum sulfate, diethanolamine, a pH regulator, a complexing agent, Tween 20, and water, aluminum sulfate accounts for 56%-58%, diethanolamine accounts for 5%-6%, the pH regulator accounts for 0.7%-0.8%, the complexing agent accounts for 1.3%-1.4%, Tween 20 accounts for 0.6%-0.8%, and the remainder is water. The preparation method comprises: after uniformly mixing water, a pH regulator, and a complexing agent, adding the mixture into a reaction kettle, and heating the reaction kettle; adding aluminum sulfate into the reaction kettle, and stirring the mixture until the aluminum sulfate is completely dissolved; adding diethanolamine into the reaction kettle to obtain a premix; and adding tween 20 into the premix to obtain a liquid accelerator. The liquid accelerator prepared in the present invention also achieves the effect of being free of alkali, chlorine, and fluorine while ensuring the effects of rapid setting, early strength, and stability.
La présente invention concerne un procédé de préparation d'un accélérateur liquide de résistance précoce, exempt d'alcali, de chlore et de fluor. En pourcentage en masse et sur la base de la somme des quantités d'utilisation de sulfate d'aluminium, de diéthanolamine, d'un régulateur de pH, d'un agent complexant, de Tween 20 et d'eau, le sulfate d'aluminium représente 56 % à 58 %, la diéthanolamine représente 5 % à 6 %, le régulateur de pH représente 0,7 % à 0,8 %, l'agent complexant représente 1,3 % à 1,4 %, Tween 20 représente 0,6 % à 0,8 %, et le reste est de l'eau. Le procédé de préparation comprend : après le mélange uniforme d'eau, d'un régulateur de pH et d'un agent complexant, l'addition du mélange dans une cuve de réaction, et le chauffage de la cuve de réaction ; l'addition de sulfate d'aluminium dans la cuve de réaction, et l'agitation du mélange jusqu'à ce que le sulfate d'aluminium soit complètement dissous ; l'addition de diéthanolamine dans la cuve de réaction pour obtenir un prémélange ; et l'addition de Tween 20 dans le prémélange pour obtenir un accélérateur liquide. L'accélérateur liquide préparé dans la présente invention permet également d'atteindre l'effet d'être exempt d'alcali, de chlore et de fluor tout en assurant les effets d'un durcissement rapide, d'une résistance précoce et d'une stabilité.
本发明提供了一种制备无碱无氯无氟早强型液体速凝剂的方法,以质量百分含量计,以硫酸铝、二乙醇胺、pH调节剂、络合剂、吐温20和水的用量之和为基准,硫酸铝的用量为56%~58%,二乙醇胺的用量为5%~6%,pH调节剂的用量为0.7%~0.8%,络合剂的用量为1.3%~1.4%,吐温20的用量为0.6%~0.8%,余量为水;该制备方法包括将水、pH调节剂和络合剂混匀后加入反应釜中,并加热反应釜;将硫酸铝加入所述反应釜中搅拌至完全溶解;将二乙醇胺加入所述反应釜中得到预混料;向所述预混料中加入吐温20制得液体速凝剂。本发明所制备的液体速凝剂在保证速凝、早强和稳定性的效果下,也实现了无碱无氯无氟的效果。
METHOD FOR PREPARING EARLY-STRENGTH LIQUID ACCELERATOR FREE OF ALKALI, CHLORINE, AND FLUORINE
The present invention provides a method for preparing an early-strength liquid accelerator free of alkali, chlorine, and fluorine. In percentage by mass and on the basis of the sum of the usage amounts of aluminum sulfate, diethanolamine, a pH regulator, a complexing agent, Tween 20, and water, aluminum sulfate accounts for 56%-58%, diethanolamine accounts for 5%-6%, the pH regulator accounts for 0.7%-0.8%, the complexing agent accounts for 1.3%-1.4%, Tween 20 accounts for 0.6%-0.8%, and the remainder is water. The preparation method comprises: after uniformly mixing water, a pH regulator, and a complexing agent, adding the mixture into a reaction kettle, and heating the reaction kettle; adding aluminum sulfate into the reaction kettle, and stirring the mixture until the aluminum sulfate is completely dissolved; adding diethanolamine into the reaction kettle to obtain a premix; and adding tween 20 into the premix to obtain a liquid accelerator. The liquid accelerator prepared in the present invention also achieves the effect of being free of alkali, chlorine, and fluorine while ensuring the effects of rapid setting, early strength, and stability.
La présente invention concerne un procédé de préparation d'un accélérateur liquide de résistance précoce, exempt d'alcali, de chlore et de fluor. En pourcentage en masse et sur la base de la somme des quantités d'utilisation de sulfate d'aluminium, de diéthanolamine, d'un régulateur de pH, d'un agent complexant, de Tween 20 et d'eau, le sulfate d'aluminium représente 56 % à 58 %, la diéthanolamine représente 5 % à 6 %, le régulateur de pH représente 0,7 % à 0,8 %, l'agent complexant représente 1,3 % à 1,4 %, Tween 20 représente 0,6 % à 0,8 %, et le reste est de l'eau. Le procédé de préparation comprend : après le mélange uniforme d'eau, d'un régulateur de pH et d'un agent complexant, l'addition du mélange dans une cuve de réaction, et le chauffage de la cuve de réaction ; l'addition de sulfate d'aluminium dans la cuve de réaction, et l'agitation du mélange jusqu'à ce que le sulfate d'aluminium soit complètement dissous ; l'addition de diéthanolamine dans la cuve de réaction pour obtenir un prémélange ; et l'addition de Tween 20 dans le prémélange pour obtenir un accélérateur liquide. L'accélérateur liquide préparé dans la présente invention permet également d'atteindre l'effet d'être exempt d'alcali, de chlore et de fluor tout en assurant les effets d'un durcissement rapide, d'une résistance précoce et d'une stabilité.
本发明提供了一种制备无碱无氯无氟早强型液体速凝剂的方法,以质量百分含量计,以硫酸铝、二乙醇胺、pH调节剂、络合剂、吐温20和水的用量之和为基准,硫酸铝的用量为56%~58%,二乙醇胺的用量为5%~6%,pH调节剂的用量为0.7%~0.8%,络合剂的用量为1.3%~1.4%,吐温20的用量为0.6%~0.8%,余量为水;该制备方法包括将水、pH调节剂和络合剂混匀后加入反应釜中,并加热反应釜;将硫酸铝加入所述反应釜中搅拌至完全溶解;将二乙醇胺加入所述反应釜中得到预混料;向所述预混料中加入吐温20制得液体速凝剂。本发明所制备的液体速凝剂在保证速凝、早强和稳定性的效果下,也实现了无碱无氯无氟的效果。
METHOD FOR PREPARING EARLY-STRENGTH LIQUID ACCELERATOR FREE OF ALKALI, CHLORINE, AND FLUORINE
PROCÉDÉ DE PRÉPARATION D'UN ACCÉLÉRATEUR LIQUIDE DE RÉSISTANCE PRÉCOCE, EXEMPT D'ALCALI, DE CHLORE ET DE FLUOR
一种制备无碱无氯无氟早强型液体速凝剂的方法
YUAN QIANG (author) / TIAN YI (author) / YANG QIAN (author) / HU CHAOLONG (author) / CHEN LEI (author) / YU ZHIWU (author) / TAN SUI (author)
2024-05-10
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Alkali-free, chlorine-free and fluorine-free liquid accelerator, application and concrete
European Patent Office | 2023
|Alkali-free fluorine-free chlorine-free liquid concrete accelerator and preparation method thereof
European Patent Office | 2022
|European Patent Office | 2025
|European Patent Office | 2024
|European Patent Office | 2021
|