Effect of the Flexural Strength on Finger-Jointed Wood with 25 mm Finger Length and 19 mm Finger Length
Timber is a renewable resource and is widely used for furniture manufacturing and construction industry in the world. Finger Joint is an effective method to minimize the timber wastage arising in the timber-related industries. This study was undertaken to effect of the bending test on finger-jointed wood with 25 mm finger length and 19 mm finger length. For bonding purposes, SWR adhesive (PVAc) D3-type glue was used at normal exposure conditions. Well-seasoned, defect-free wood materials from seven timber species; Grandis, Jack, Kumbuk, Mahogany, Pine, Satin, and Teak were selected for this study. BS 373:1957 was used as a standard for tests. Mechanical properties were performed by the Universal Testing Machine (UTM 100PC). Results were analyzed using ANOVA. Results revealed that there is a significant relationship between MOR and finger length (P < 0.05) and there is no significant relationship between MOE and finger length (P > 0.05) and can be recommended, horizontally oriented 19 mm finger-jointed specimens suitable for finger joint applications than 25 mm finger-jointed specimens.
Effect of the Flexural Strength on Finger-Jointed Wood with 25 mm Finger Length and 19 mm Finger Length
Timber is a renewable resource and is widely used for furniture manufacturing and construction industry in the world. Finger Joint is an effective method to minimize the timber wastage arising in the timber-related industries. This study was undertaken to effect of the bending test on finger-jointed wood with 25 mm finger length and 19 mm finger length. For bonding purposes, SWR adhesive (PVAc) D3-type glue was used at normal exposure conditions. Well-seasoned, defect-free wood materials from seven timber species; Grandis, Jack, Kumbuk, Mahogany, Pine, Satin, and Teak were selected for this study. BS 373:1957 was used as a standard for tests. Mechanical properties were performed by the Universal Testing Machine (UTM 100PC). Results were analyzed using ANOVA. Results revealed that there is a significant relationship between MOR and finger length (P < 0.05) and there is no significant relationship between MOE and finger length (P > 0.05) and can be recommended, horizontally oriented 19 mm finger-jointed specimens suitable for finger joint applications than 25 mm finger-jointed specimens.
Effect of the Flexural Strength on Finger-Jointed Wood with 25 mm Finger Length and 19 mm Finger Length
Lecture Notes in Civil Engineering
Dissanayake, Ranjith (editor) / Mendis, Priyan (editor) / De Silva, Sudhira (editor) / Fernando, Shiromal (editor) / Konthesingha, Chaminda (editor) / Attanayake, Upul (editor) / Gajanayake, Pradeep (editor) / Muthumala, C. K. (author) / Abeysekara, K. D. A. (author) / Alwis, P. L. A. G. (author)
International Conference on Sustainable Built Environment ; 2023 ; Kandy, Sri Lanka
Proceedings of the 14th International Conference on Sustainable Built Environment ; Chapter: 7 ; 81-89
2024-08-28
9 pages
Article/Chapter (Book)
Electronic Resource
English
Engineering Index Backfile | 1966
|Finger-jointed beams in bending
British Library Conference Proceedings | 1997
|The effect of acetylation on bending strength of finger jointed beech wood (Fagus sylvatica L.)
British Library Online Contents | 2008
|Use of Finger-Jointed Timber in Housing
Springer Verlag | 1982
|