The invention relates to water seepage prevention cement which is prepared from the following raw materials in percentage by weight: 5%-8% of fluorine-containing polyacrylate latex powder, 2%-3% of rosin of 100-200 meshes, 3%-5% of sodium silicate, 3%-5% of calcium hydroxide, 1%-2% of alums, 1%-2% of sodium dodecyl sulfate, 10%-15% of sulphate aluminum cement and the balance of silicate cement, wherein the fluorine content of the fluorine-containing polyacrylate latex powder is 1%-3%. The water seepage prevention cement prepared by the invention has water seepage prevention function.
The invention relates to water seepage prevention cement which is prepared from the following raw materials in percentage by weight: 5%-8% of fluorine-containing polyacrylate latex powder, 2%-3% of rosin of 100-200 meshes, 3%-5% of sodium silicate, 3%-5% of calcium hydroxide, 1%-2% of alums, 1%-2% of sodium dodecyl sulfate, 10%-15% of sulphate aluminum cement and the balance of silicate cement, wherein the fluorine content of the fluorine-containing polyacrylate latex powder is 1%-3%. The water seepage prevention cement prepared by the invention has water seepage prevention function.
Water seepage prevention cement
LI YONGQIAN (Autor:in)
03.06.2015
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME
Basement water seepage prevention structure and basement water seepage prevention treatment method
Europäisches Patentamt | 2020
|Europäisches Patentamt | 2022
|