High-strength permeable pavement
The invention discloses a high-strength water permeable pavement which is formed by piling with a binding material. The binding material is composed of the following components in parts by mass: 25-35parts of sintered corundum, 40-50 parts of silica sol, 3-5 parts of sodium tripolyphosphate, 4-6 parts of polyphosphate, 5 to 8 parts of dioctyl phthalate; 12-15 parts of rosin modified phenolic resin; 10-15 parts of carbon fibers, 30-40 parts of furfural oil, 25-30 parts of terpene resin; 3-5 parts of calcium chloride, 2-4 parts of ethylene glycol, 3-5 parts of methyl silicone oil, 6 parts of sodium silicate, 2 parts of chlorinated paraffin, 2 parts of chlorinated rubber, 6-10 parts of glass fibers, 0.5-1 part of a thickening agent, 20 parts of aluminum silicate fibers, 3 parts of sodium aluminum phosphate, 15 parts of limestone powder, 14-18 parts of sodium lignin sulfonate, 5-8 parts of alkyl silicate, 20-30 parts of trimethyloltriacrylate and 20-30 parts of water. The binding materialused for the permeable pavement can enhance the contact area between aggregates of the permeable pavement, thereby enhancing the strength of the permeable pavement.
本发明公开了一种高强度透水路面,通过粘结材料堆砌而成,粘结材料由如下质量份数的组分组成:25~35份烧结刚玉、40~50份硅溶胶、3~5份三聚磷酸钠、4~6份、多聚磷酸酯、5~8份邻苯二甲酸二辛酯、12~15份松香改性酚醛树脂、10~15份碳纤维、30~40份糠醛油、25~30份萜烯树脂、3~5份氯化钙、2~4份乙二醇、3~5份甲基硅油、6份硅酸钠、2份氯化石蜡、2份氯化橡胶、6~10份玻璃纤维、0.5~1份增稠剂、20份硅酸铝纤维、3份磷酸铝钠、15份石灰石粉、14~18份木质素磺酸钠、5~8份硅酸烷基酯、20~30份三羟甲基三丙烯酸酯以及20~30份水。本发明透水路面使用的粘结材料能够增强透水路面集料与集料之间的接触面积,从而提高透水路面的强度。
High-strength permeable pavement
The invention discloses a high-strength water permeable pavement which is formed by piling with a binding material. The binding material is composed of the following components in parts by mass: 25-35parts of sintered corundum, 40-50 parts of silica sol, 3-5 parts of sodium tripolyphosphate, 4-6 parts of polyphosphate, 5 to 8 parts of dioctyl phthalate; 12-15 parts of rosin modified phenolic resin; 10-15 parts of carbon fibers, 30-40 parts of furfural oil, 25-30 parts of terpene resin; 3-5 parts of calcium chloride, 2-4 parts of ethylene glycol, 3-5 parts of methyl silicone oil, 6 parts of sodium silicate, 2 parts of chlorinated paraffin, 2 parts of chlorinated rubber, 6-10 parts of glass fibers, 0.5-1 part of a thickening agent, 20 parts of aluminum silicate fibers, 3 parts of sodium aluminum phosphate, 15 parts of limestone powder, 14-18 parts of sodium lignin sulfonate, 5-8 parts of alkyl silicate, 20-30 parts of trimethyloltriacrylate and 20-30 parts of water. The binding materialused for the permeable pavement can enhance the contact area between aggregates of the permeable pavement, thereby enhancing the strength of the permeable pavement.
本发明公开了一种高强度透水路面,通过粘结材料堆砌而成,粘结材料由如下质量份数的组分组成:25~35份烧结刚玉、40~50份硅溶胶、3~5份三聚磷酸钠、4~6份、多聚磷酸酯、5~8份邻苯二甲酸二辛酯、12~15份松香改性酚醛树脂、10~15份碳纤维、30~40份糠醛油、25~30份萜烯树脂、3~5份氯化钙、2~4份乙二醇、3~5份甲基硅油、6份硅酸钠、2份氯化石蜡、2份氯化橡胶、6~10份玻璃纤维、0.5~1份增稠剂、20份硅酸铝纤维、3份磷酸铝钠、15份石灰石粉、14~18份木质素磺酸钠、5~8份硅酸烷基酯、20~30份三羟甲基三丙烯酸酯以及20~30份水。本发明透水路面使用的粘结材料能够增强透水路面集料与集料之间的接触面积,从而提高透水路面的强度。
High-strength permeable pavement
一种高强度透水路面
WEI TANGZHONG (Autor:in) / LI PEINING (Autor:in) / XIA XINJIE (Autor:in) / LU WANHUA (Autor:in)
21.04.2020
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME