Preparation method of foamed light soil, and foamed light soil
The invention discloses a preparation method of foamed light soil, and the foamed light soil. The foamed light soil comprises, by mass, 25-40% of an admixture, 40-65% of a cementing material, 3-21% ofa chemical auxiliary agent, 1-5% of an active silica-alumina substance material and camphanone-2 powder; and the cementing material comprises cement clinker, calcium oxide and bone glue powder, and the mass ratio of the three components in the cementing material is 2: 3: 1. The invention also discloses a preparation method of the foamed light soil. The preparation method comprises the following steps: premixing the raw materials; preparing a slurry; adding a foaming agent; forming a green body; and drying. The energy utilization shortage is effectively relieved, and the foamed light soil is high in strength, less in moisture, quick to dry, good in bonding and shaping and convenient to use.
本发明公开了一种泡沫轻质土的制备方法及泡沫轻质土,该泡沫轻质土包括外掺料、胶结材料、化学辅助剂、活性硅铝物质材料、莰酮-2粉末剂,包括:外掺料的质量占比为25%至40%;胶结材料的质量占比40%至65%;化学辅助剂的质量占比为3%至21%;活性硅铝物质材料的质量占比为1%至5%;所述胶结材料包括水泥熟料、氧化钙和骨胶粉,所述三种成分在胶结材料中的质量比为2:3:1。本发明还公开了一种泡沫轻质土的制备方法,包括:原料预混合;料浆制备;加入发泡剂;生坯成型;干燥。通过本发明实施例有效缓解了紧张的能源利用,还可以使泡沫轻质土强度高,水分少,干燥快,黏结定型好,使用方便。
Preparation method of foamed light soil, and foamed light soil
The invention discloses a preparation method of foamed light soil, and the foamed light soil. The foamed light soil comprises, by mass, 25-40% of an admixture, 40-65% of a cementing material, 3-21% ofa chemical auxiliary agent, 1-5% of an active silica-alumina substance material and camphanone-2 powder; and the cementing material comprises cement clinker, calcium oxide and bone glue powder, and the mass ratio of the three components in the cementing material is 2: 3: 1. The invention also discloses a preparation method of the foamed light soil. The preparation method comprises the following steps: premixing the raw materials; preparing a slurry; adding a foaming agent; forming a green body; and drying. The energy utilization shortage is effectively relieved, and the foamed light soil is high in strength, less in moisture, quick to dry, good in bonding and shaping and convenient to use.
本发明公开了一种泡沫轻质土的制备方法及泡沫轻质土,该泡沫轻质土包括外掺料、胶结材料、化学辅助剂、活性硅铝物质材料、莰酮-2粉末剂,包括:外掺料的质量占比为25%至40%;胶结材料的质量占比40%至65%;化学辅助剂的质量占比为3%至21%;活性硅铝物质材料的质量占比为1%至5%;所述胶结材料包括水泥熟料、氧化钙和骨胶粉,所述三种成分在胶结材料中的质量比为2:3:1。本发明还公开了一种泡沫轻质土的制备方法,包括:原料预混合;料浆制备;加入发泡剂;生坯成型;干燥。通过本发明实施例有效缓解了紧张的能源利用,还可以使泡沫轻质土强度高,水分少,干燥快,黏结定型好,使用方便。
Preparation method of foamed light soil, and foamed light soil
一种泡沫轻质土的制备方法及泡沫轻质土
CHEN ZHONGPING (Autor:in)
02.06.2020
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2021
|Europäisches Patentamt | 2024
|Europäisches Patentamt | 2024
|Europäisches Patentamt | 2022
|