Environment-friendly aluminum-magnesium-chromium high-performance anhydrous stemming and preparation method thereof
The invention provides environment-friendly aluminum-magnesium-chromium high-performance anhydrous stemming. The environment-friendly aluminum-magnesium-chromium high-performance anhydrous stemming comprises the following components in parts by weight: aggregate consisting of 2-5 parts of kyanite, 15 to 20 parts of high-alumina bauxite, 15-20 parts of an aluminum-chromium material, 15-20 parts ofa magnesium carbon material, 6-10 parts of coke and 13-16 parts of a corundum carbon composite material; micro-powder consisting of 5-10 parts of Guangxi white mud, 5-8 parts of sericite and 3-6 partsof silicon carbide; and a binding agent consisting of 3-6 parts of modified asphalt, 2-4 parts of modified resin and 10 to 15 parts of modified tar. In addition, the invention also provides a preparation method of the anhydrous stemming. The method is simple to operate and mild in preparation process.
本发明提供一种环保型铝镁铬质高性能无水炮泥,包括如下重量份的组分:骨料:蓝晶石2‑5;高铝钒土15‑20;铝铬材料15‑20;镁碳料15‑20;焦炭6‑10;钢玉碳复合料13‑16;微粉:广西白泥5‑10;绢云母5‑8;碳化硅3‑6;结合剂:改性沥青3‑6;改性树脂2‑4;改性焦油10‑15;另外,本发明还提供了上述无水炮泥的制备方法,该方法操作简单,制备工艺温和。
Environment-friendly aluminum-magnesium-chromium high-performance anhydrous stemming and preparation method thereof
The invention provides environment-friendly aluminum-magnesium-chromium high-performance anhydrous stemming. The environment-friendly aluminum-magnesium-chromium high-performance anhydrous stemming comprises the following components in parts by weight: aggregate consisting of 2-5 parts of kyanite, 15 to 20 parts of high-alumina bauxite, 15-20 parts of an aluminum-chromium material, 15-20 parts ofa magnesium carbon material, 6-10 parts of coke and 13-16 parts of a corundum carbon composite material; micro-powder consisting of 5-10 parts of Guangxi white mud, 5-8 parts of sericite and 3-6 partsof silicon carbide; and a binding agent consisting of 3-6 parts of modified asphalt, 2-4 parts of modified resin and 10 to 15 parts of modified tar. In addition, the invention also provides a preparation method of the anhydrous stemming. The method is simple to operate and mild in preparation process.
本发明提供一种环保型铝镁铬质高性能无水炮泥,包括如下重量份的组分:骨料:蓝晶石2‑5;高铝钒土15‑20;铝铬材料15‑20;镁碳料15‑20;焦炭6‑10;钢玉碳复合料13‑16;微粉:广西白泥5‑10;绢云母5‑8;碳化硅3‑6;结合剂:改性沥青3‑6;改性树脂2‑4;改性焦油10‑15;另外,本发明还提供了上述无水炮泥的制备方法,该方法操作简单,制备工艺温和。
Environment-friendly aluminum-magnesium-chromium high-performance anhydrous stemming and preparation method thereof
一种环保型铝镁铬质高性能无水炮泥及制备方法
HAO JIANGUO (Autor:in) / MENG LI (Autor:in) / JIANG YAOQING (Autor:in)
29.09.2020
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Preparation method of environment-friendly anhydrous stemming
Europäisches Patentamt | 2024
|Environment-friendly high-strength anhydrous stemming and preparation method thereof
Europäisches Patentamt | 2021
|Anti-splashing environment-friendly anhydrous stemming
Europäisches Patentamt | 2021
|