The invention provides a lightweight environment-friendly building material and a preparation method thereof, and relates to the technical field of building materials. The light environment-friendly building material comprises , by weight, 30-50 parts of magnesium oxychloride cement, 1-3 parts of citric acid, 5-10 parts of straws, 3-5 parts of wood flour, 3-5 parts of basic magnesium sulfate whiskers, 5-10 parts of a modifier, 3-5 parts of modified rubber powder, 2-5 parts of termite mud, 2-5 parts of a composite foaming agent, 1-3 parts of a water reducing agent and 1-2 parts of glucose. The properties of the magnesium oxychloride cement are improved through the components, so that the water resistance, the stability and the mechanical strength of the prepared lightweight environment-friendly building material are improved, the performance of the components is better than that of traditional used materials, the foaming performance of the lightweight environment-friendly building material prepared from the magnesium oxychloride cement is improved, and meanwhile, the interface strength is improved. In addition, the termite mud is used as a reinforcing agent and a termite-proof agent, and is more environment-friendly compared with direct use of the termite-proof agent.
本发明提供一种轻质环保建筑材料及其制备方法,涉及建筑材料技术领域。该轻质环保建筑材料,包括以下重量分成份组成:30~50份氯氧镁水泥、1~3份柠檬酸、5~10份秸秆、3~5份木粉、3~5份碱式硫酸镁晶须、5~10份改性剂、3~5份改性橡胶粉、2~5份白蚁坭、2~5份复合发泡剂、1~3份减水剂、1~2份葡萄糖。通过各组分对氯氧镁水泥的性质进行改良,使得制成的轻质环保建筑材料,在耐水性、稳定性和力学强度都得到了提高,各组分相较于传统使用材料性能更优,使氯氧镁水泥制成的轻质环保建筑材料兼顾泡发性能提高的同时,界面强度提高,此外使用白蚁坭作为增强剂和防白蚁剂,相对于直接使用防白蚁剂更加环保。
The invention provides a lightweight environment-friendly building material and a preparation method thereof, and relates to the technical field of building materials. The light environment-friendly building material comprises , by weight, 30-50 parts of magnesium oxychloride cement, 1-3 parts of citric acid, 5-10 parts of straws, 3-5 parts of wood flour, 3-5 parts of basic magnesium sulfate whiskers, 5-10 parts of a modifier, 3-5 parts of modified rubber powder, 2-5 parts of termite mud, 2-5 parts of a composite foaming agent, 1-3 parts of a water reducing agent and 1-2 parts of glucose. The properties of the magnesium oxychloride cement are improved through the components, so that the water resistance, the stability and the mechanical strength of the prepared lightweight environment-friendly building material are improved, the performance of the components is better than that of traditional used materials, the foaming performance of the lightweight environment-friendly building material prepared from the magnesium oxychloride cement is improved, and meanwhile, the interface strength is improved. In addition, the termite mud is used as a reinforcing agent and a termite-proof agent, and is more environment-friendly compared with direct use of the termite-proof agent.
本发明提供一种轻质环保建筑材料及其制备方法,涉及建筑材料技术领域。该轻质环保建筑材料,包括以下重量分成份组成:30~50份氯氧镁水泥、1~3份柠檬酸、5~10份秸秆、3~5份木粉、3~5份碱式硫酸镁晶须、5~10份改性剂、3~5份改性橡胶粉、2~5份白蚁坭、2~5份复合发泡剂、1~3份减水剂、1~2份葡萄糖。通过各组分对氯氧镁水泥的性质进行改良,使得制成的轻质环保建筑材料,在耐水性、稳定性和力学强度都得到了提高,各组分相较于传统使用材料性能更优,使氯氧镁水泥制成的轻质环保建筑材料兼顾泡发性能提高的同时,界面强度提高,此外使用白蚁坭作为增强剂和防白蚁剂,相对于直接使用防白蚁剂更加环保。
Environment-friendly building material and preparation method thereof
Europäisches Patentamt | 2020
|Europäisches Patentamt | 2023
|Environment-friendly lightweight elastic layer polyurethane material and preparation method thereof
Europäisches Patentamt | 2023
|Environment-friendly lightweight concrete and preparation method thereof
Europäisches Patentamt | 2024
|Environment-friendly lightweight concrete and preparation method thereof
Europäisches Patentamt | 2020
|