The invention provides a hollow slab bridge hinge joint repairing method without interrupting traffic, and relates to the technical field of bridge hinge joint repairing. The method for repairing the hinge joint of the hollow slab bridge without interrupting the traffic mainly comprises the following steps that the end of a slab joint is clamped through battens, the bottom of the slab joint is connected with the top of the slab joint to seal the beam end, glue injection pipes and observation pipes are arranged between the battens at the two ends in a paired mode every 1.5-2 m, and then the bottom of the slab joint is sealed; and one-time glue injection and curing are carried out on 0-3 mm plate joints through a glue injection pipe after the plate joints are filled with glue. The method has the advantages that the construction period is short, traffic interruption is not needed, vehicle congestion is not caused, the original structure of the bridge is not affected, consumed manpower and material resources are few, and good economical efficiency is achieved.
本发明提出一种不中断交通空心板桥梁铰缝修复方法,涉及桥梁铰缝修复技术领域。此不中断交通空心板桥梁铰缝修复方法主要包括以下步骤:将板缝端部用木条卡紧且其底部与板缝的顶部相接以封闭梁端,两端木条之间每相隔1.5‑2米配对设置注胶管与观测管,然后将板缝封底;0‑3毫米的板缝通过注胶管进行一次注胶注满固化即可。该方法具有施工周期短、不需中断交通、不会造成车辆拥堵,对桥梁原有结构无影响的优点,消耗的人力物力少,具有较好的经济性。
The invention provides a hollow slab bridge hinge joint repairing method without interrupting traffic, and relates to the technical field of bridge hinge joint repairing. The method for repairing the hinge joint of the hollow slab bridge without interrupting the traffic mainly comprises the following steps that the end of a slab joint is clamped through battens, the bottom of the slab joint is connected with the top of the slab joint to seal the beam end, glue injection pipes and observation pipes are arranged between the battens at the two ends in a paired mode every 1.5-2 m, and then the bottom of the slab joint is sealed; and one-time glue injection and curing are carried out on 0-3 mm plate joints through a glue injection pipe after the plate joints are filled with glue. The method has the advantages that the construction period is short, traffic interruption is not needed, vehicle congestion is not caused, the original structure of the bridge is not affected, consumed manpower and material resources are few, and good economical efficiency is achieved.
本发明提出一种不中断交通空心板桥梁铰缝修复方法,涉及桥梁铰缝修复技术领域。此不中断交通空心板桥梁铰缝修复方法主要包括以下步骤:将板缝端部用木条卡紧且其底部与板缝的顶部相接以封闭梁端,两端木条之间每相隔1.5‑2米配对设置注胶管与观测管,然后将板缝封底;0‑3毫米的板缝通过注胶管进行一次注胶注满固化即可。该方法具有施工周期短、不需中断交通、不会造成车辆拥堵,对桥梁原有结构无影响的优点,消耗的人力物力少,具有较好的经济性。
Method for repairing hinge joint of hollow slab bridge without interrupting traffic
一种不中断交通空心板桥梁铰缝修复方法
YANG BIN (Autor:in)
03.09.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
E01D
BRIDGES
,
Brücken
Concrete hollow slab beam shear-resistant reinforcing method without interrupting traffic
Europäisches Patentamt | 2023
|Hollow slab beam hinge joint water seepage repairing structure and method
Europäisches Patentamt | 2023
|Europäisches Patentamt | 2015
|Reinforcing method for hinge joint of hollow slab of bridge
Europäisches Patentamt | 2023
|Europäisches Patentamt | 2020
|