Ceramic building block and preparation method thereof
The invention relates to the technical field of building materials, and particularly discloses a ceramic building block and a preparation method thereof. The ceramic building block comprises the following components in parts by mass: 45-65 parts of ceramic coarse aggregate, 45-58 parts of ceramic fine aggregate, 20-25 parts of ground ceramic powder, 20-25 parts of sodium silicate and 8-12 parts of water. According to the ceramic building block provided by the invention, ceramic is used as a main raw material, under the condition that traditional components such as cement, sand and lime are not added, only three ceramic raw materials with different particle sizes and proportions are compatible, and a conventional curing process is performed under the action of sodium silicate, so that relatively high use strength can be achieved, and addition of cement is omitted; and the manufacturing cost of the building block is effectively reduced.
本发明涉及建筑材料技术领域,具体公开一种陶瓷砌块及其制备方法。所述陶瓷砌块包括以下质量份数的组分:陶瓷粗骨料45‑65份,陶瓷细骨料45‑58份,磨细陶瓷粉20‑25份,硅酸钠20‑25份和水8‑12份。本发明提供的陶瓷砌块以陶瓷为主要原料,在不加入水泥、砂和石灰等传统成分的情况下,仅通过将三种不同粒径和比例的陶瓷原料进行配伍,在硅酸钠的作用下进行常规的养护过程,即可达到较高的使用强度,且省去了水泥的添加,有效降低了建筑砌块的制作成本。
Ceramic building block and preparation method thereof
The invention relates to the technical field of building materials, and particularly discloses a ceramic building block and a preparation method thereof. The ceramic building block comprises the following components in parts by mass: 45-65 parts of ceramic coarse aggregate, 45-58 parts of ceramic fine aggregate, 20-25 parts of ground ceramic powder, 20-25 parts of sodium silicate and 8-12 parts of water. According to the ceramic building block provided by the invention, ceramic is used as a main raw material, under the condition that traditional components such as cement, sand and lime are not added, only three ceramic raw materials with different particle sizes and proportions are compatible, and a conventional curing process is performed under the action of sodium silicate, so that relatively high use strength can be achieved, and addition of cement is omitted; and the manufacturing cost of the building block is effectively reduced.
本发明涉及建筑材料技术领域,具体公开一种陶瓷砌块及其制备方法。所述陶瓷砌块包括以下质量份数的组分:陶瓷粗骨料45‑65份,陶瓷细骨料45‑58份,磨细陶瓷粉20‑25份,硅酸钠20‑25份和水8‑12份。本发明提供的陶瓷砌块以陶瓷为主要原料,在不加入水泥、砂和石灰等传统成分的情况下,仅通过将三种不同粒径和比例的陶瓷原料进行配伍,在硅酸钠的作用下进行常规的养护过程,即可达到较高的使用强度,且省去了水泥的添加,有效降低了建筑砌块的制作成本。
Ceramic building block and preparation method thereof
一种陶瓷砌块及其制备方法
WU LIPENG (Autor:in) / LI XUANHAO (Autor:in) / LI ZHENGZHENG (Autor:in) / ZHOU YONGXIANG (Autor:in)
22.03.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Foamed ceramic building block as well as preparation method and use method thereof
Europäisches Patentamt | 2023
|Building ceramic plate and preparation method thereof
Europäisches Patentamt | 2024
|Ceramic building material and preparation method thereof
Europäisches Patentamt | 2022
|