Lightweight gypsum spraying mortar and preparation method thereof
The invention provides light gypsum spraying mortar and a preparation method thereof. The light gypsum spraying mortar is prepared from the following raw materials in parts by weight: 60-70 parts of phosphogypsum, 0.8-1.2 parts of quick lime, 6-15 parts of sepiolite/fly ash composite modified material, 6-15 parts of Portland cement, 0.8-1.5 parts of aluminum dihydrogen phosphate, 1-5 parts of quartz sand and 0.1-0.2 part of sodium citrate, the phosphogypsum is subjected to surface modification through the quick lime, so that the waterproof performance is improved; and the setting time and the mechanical property of the base material can be prolonged, so that the construction requirements are met. By adding the sepiolite/fly ash composite modified material, Portland cement, aluminum dihydrogen phosphate and sodium citrate, the activity is excited in the hydration reaction process, a cementing material is formed, and the later strength is improved.
本发明提供一种轻质石膏喷涂砂浆及其制备方法,由以下重量份的原料组成:磷石膏60~70份、生石灰0.8~1.2份、海泡石/粉煤灰复合改性材料6~15份、硅酸盐水泥6~15份、双氢磷酸铝0.8~1.5份、石英砂1~5份、柠檬酸钠0.1~0.2份;本发明通过生石灰对磷石膏进行表面改性,提高防水性能;且还能够延长基体材料的凝结时间和力学性能,以满足施工要求。通过添加海泡石/粉煤灰复合改性材料、硅酸盐水泥、双氢磷酸铝和柠檬酸钠,在水化反应的过程中激发活性,形成胶凝材料,提高后期强度。
Lightweight gypsum spraying mortar and preparation method thereof
The invention provides light gypsum spraying mortar and a preparation method thereof. The light gypsum spraying mortar is prepared from the following raw materials in parts by weight: 60-70 parts of phosphogypsum, 0.8-1.2 parts of quick lime, 6-15 parts of sepiolite/fly ash composite modified material, 6-15 parts of Portland cement, 0.8-1.5 parts of aluminum dihydrogen phosphate, 1-5 parts of quartz sand and 0.1-0.2 part of sodium citrate, the phosphogypsum is subjected to surface modification through the quick lime, so that the waterproof performance is improved; and the setting time and the mechanical property of the base material can be prolonged, so that the construction requirements are met. By adding the sepiolite/fly ash composite modified material, Portland cement, aluminum dihydrogen phosphate and sodium citrate, the activity is excited in the hydration reaction process, a cementing material is formed, and the later strength is improved.
本发明提供一种轻质石膏喷涂砂浆及其制备方法,由以下重量份的原料组成:磷石膏60~70份、生石灰0.8~1.2份、海泡石/粉煤灰复合改性材料6~15份、硅酸盐水泥6~15份、双氢磷酸铝0.8~1.5份、石英砂1~5份、柠檬酸钠0.1~0.2份;本发明通过生石灰对磷石膏进行表面改性,提高防水性能;且还能够延长基体材料的凝结时间和力学性能,以满足施工要求。通过添加海泡石/粉煤灰复合改性材料、硅酸盐水泥、双氢磷酸铝和柠檬酸钠,在水化反应的过程中激发活性,形成胶凝材料,提高后期强度。
Lightweight gypsum spraying mortar and preparation method thereof
一种轻质石膏喷涂砂浆及其制备方法
LI XINGZHEN (Autor:in) / CHENG CHENG (Autor:in)
26.07.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Lightweight gypsum mortar and preparation method thereof
Europäisches Patentamt | 2021
|Lightweight plastering gypsum mortar and preparation method thereof
Europäisches Patentamt | 2021
|Lightweight plastering gypsum mortar and preparation method thereof
Europäisches Patentamt | 2023
|Lightweight plastering gypsum mortar and preparation method thereof
Europäisches Patentamt | 2023
|Lightweight plastering gypsum mortar and preparation method thereof
Europäisches Patentamt | 2021
|