The invention discloses an electric porcelain brown glaze formula suitable for tunnel kiln firing, which comprises the following raw materials in parts by mass: 20-40 parts of potassium feldspar, 10-20 parts of quartz, 5-15 parts of Yichun soil, 5-18 parts of Jiepai mud, 1-5 parts of talc, 2-8 parts of wollastonite, 5-20 parts of porcelain powder, 5-20 parts of blank mud, 1-5 parts of iron oxide red, 3-8 parts of manganese powder and 1-8 parts of green chromium, the Yichun soil is high-purity porous quartz powder with the particle size of 0.1-0.9 mu m, and is prepared by calcining crops at 900-1100 DEG C, and the burning vector of the Yichun soil is 4-6%. According to the brown glaze produced by the invention, the porcelain strength of the brown glaze can be effectively improved by more than 30%.
本发明公开了一种适用于隧道窑烧成的电瓷棕釉配方,包括以下质量份的原料:钾长石20‑40份、石英10‑20份、宜春土5‑15份、界牌泥5‑18份、滑石1‑5份、硅灰石2‑8份、瓷粉5‑20份、坯泥5‑20份、铁红1‑5份、锰粉3‑8份、绿铬1‑8份,所述石英为粉末状,且粒径为.1μm~0.9μm的高纯多孔隙石英粉,由农作物经900℃~1100℃煅烧而成,所述宜春土的烧矢量为4%~6%。通过本发明生产出的棕釉,能够有效的提高棕釉的瓷质强度30%以上。
Electric porcelain brown glaze formula suitable for tunnel kiln firing and manufacturing method thereof
The invention discloses an electric porcelain brown glaze formula suitable for tunnel kiln firing, which comprises the following raw materials in parts by mass: 20-40 parts of potassium feldspar, 10-20 parts of quartz, 5-15 parts of Yichun soil, 5-18 parts of Jiepai mud, 1-5 parts of talc, 2-8 parts of wollastonite, 5-20 parts of porcelain powder, 5-20 parts of blank mud, 1-5 parts of iron oxide red, 3-8 parts of manganese powder and 1-8 parts of green chromium, the Yichun soil is high-purity porous quartz powder with the particle size of 0.1-0.9 mu m, and is prepared by calcining crops at 900-1100 DEG C, and the burning vector of the Yichun soil is 4-6%. According to the brown glaze produced by the invention, the porcelain strength of the brown glaze can be effectively improved by more than 30%.
本发明公开了一种适用于隧道窑烧成的电瓷棕釉配方,包括以下质量份的原料:钾长石20‑40份、石英10‑20份、宜春土5‑15份、界牌泥5‑18份、滑石1‑5份、硅灰石2‑8份、瓷粉5‑20份、坯泥5‑20份、铁红1‑5份、锰粉3‑8份、绿铬1‑8份,所述石英为粉末状,且粒径为.1μm~0.9μm的高纯多孔隙石英粉,由农作物经900℃~1100℃煅烧而成,所述宜春土的烧矢量为4%~6%。通过本发明生产出的棕釉,能够有效的提高棕釉的瓷质强度30%以上。
Electric porcelain brown glaze formula suitable for tunnel kiln firing and manufacturing method thereof
一种适用于隧道窑烧成的电瓷棕釉配方及其制造方法
GAN YONG (Autor:in) / HU SHAOLIN (Autor:in) / HU YUAN (Autor:in) / XU NA (Autor:in) / LIU YU (Autor:in)
03.02.2023
Patent
Elektronische Ressource
Chinesisch
Green glaze for porcelain firing and application thereof
Europäisches Patentamt | 2024
|Electric porcelain ash glaze material, electric porcelain ash glaze and preparation thereof
Europäisches Patentamt | 2020
|Europäisches Patentamt | 2022
|High-strength siliceous brown glaze electric porcelain and preparation method thereof
Europäisches Patentamt | 2021
|