Steam pressurized concrete block and production method thereof
The invention discloses a steam pressurized concrete block and a production method thereof, and relates to the technical field of concrete blocks, the steam pressurized concrete block comprises the following raw materials by mass: 30%-40% of fly ash, 15%-20% of quick lime, 10%-20% of cement, 10%-15% of gypsum, 5%-10% of slag, 5%-10% of silica sand and auxiliary ingredients, the auxiliary ingredients comprise the following raw materials in percentage by mass: 2-5% of a fixing agent, 1-3% of a foaming agent, 2-5% of a regulator, 1-3% of a stabilizer and 2-5% of a strength improver. The strength improver is mainly water calcium silicate crystal grains, the water calcium silicate crystal grains can react to generate hydrated calcium silicate gel in a humid and hot environment, and along with the increase of the hydrated calcium silicate gel, the strength of the lime-sand brick is improved, and the situation that the steam pressurized concrete block is broken can be avoided.
本发明公开了一种蒸汽加压混凝土砌块及其生产方法,涉及混凝土砌块技术领域,包括以下质量百分比的原料组成:粉煤灰30%‑40%、生石灰15%‑20%、水泥10%‑20%、石膏10%‑15%、矿渣5%‑10%、硅砂5%‑10%和辅助配料,所述辅助配料由以下质量百分比的原料组成:固定剂2%‑5%、发气剂1%‑3%、调节剂2%‑5%、稳定剂1%‑3%和强度改善剂2%‑5%。本发明强度改善剂主要为水硅酸钙晶粒,在湿热的环境下,水硅酸钙晶粒会发生反应生成水化硅酸钙凝胶,随着水化硅酸钙凝胶的增多,从而提高了灰砂砖的强度,可避免蒸汽加压混凝土砌块碎裂的情况发生。
Steam pressurized concrete block and production method thereof
The invention discloses a steam pressurized concrete block and a production method thereof, and relates to the technical field of concrete blocks, the steam pressurized concrete block comprises the following raw materials by mass: 30%-40% of fly ash, 15%-20% of quick lime, 10%-20% of cement, 10%-15% of gypsum, 5%-10% of slag, 5%-10% of silica sand and auxiliary ingredients, the auxiliary ingredients comprise the following raw materials in percentage by mass: 2-5% of a fixing agent, 1-3% of a foaming agent, 2-5% of a regulator, 1-3% of a stabilizer and 2-5% of a strength improver. The strength improver is mainly water calcium silicate crystal grains, the water calcium silicate crystal grains can react to generate hydrated calcium silicate gel in a humid and hot environment, and along with the increase of the hydrated calcium silicate gel, the strength of the lime-sand brick is improved, and the situation that the steam pressurized concrete block is broken can be avoided.
本发明公开了一种蒸汽加压混凝土砌块及其生产方法,涉及混凝土砌块技术领域,包括以下质量百分比的原料组成:粉煤灰30%‑40%、生石灰15%‑20%、水泥10%‑20%、石膏10%‑15%、矿渣5%‑10%、硅砂5%‑10%和辅助配料,所述辅助配料由以下质量百分比的原料组成:固定剂2%‑5%、发气剂1%‑3%、调节剂2%‑5%、稳定剂1%‑3%和强度改善剂2%‑5%。本发明强度改善剂主要为水硅酸钙晶粒,在湿热的环境下,水硅酸钙晶粒会发生反应生成水化硅酸钙凝胶,随着水化硅酸钙凝胶的增多,从而提高了灰砂砖的强度,可避免蒸汽加压混凝土砌块碎裂的情况发生。
Steam pressurized concrete block and production method thereof
一种蒸汽加压混凝土砌块及其生产方法
DONG XIUMING (Autor:in)
23.06.2023
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Steam pressurized concrete block and preparation method thereof
Europäisches Patentamt | 2020
|Steam pressurized concrete block wall and construction method thereof
Europäisches Patentamt | 2020
|High-recycling steam pressurized concrete block and preparation method thereof
Europäisches Patentamt | 2016
|Steam turbine concrete cushion block production process
Europäisches Patentamt | 2015
|