The invention belongs to the technical field of high-entropy borides, and particularly relates to a preparation method of a high-entropy boride coating. The invention provides a preparation method of a high-entropy boride coating, which comprises the following steps: mixing high-entropy boride, a dispersant and a binder, and carrying out spray granulation on the obtained slurry to obtain a spherical material; sequentially carrying out first sintering and second sintering on the spherical material to obtain the high-entropy boride microspheres, and spraying the high-entropy boride microspheres serving as a coating on a matrix to obtain the high-entropy boride coating. The high-entropy boride coating obtained by the method disclosed by the invention has relatively high compactness.
本发明属于高熵硼化物技术领域,具体涉及一种高熵硼化物涂层的制备方法。本发明提供了一种高熵硼化物涂层的制备方法,包括以下步骤:将高熵硼化物、分散剂和粘结剂混合,得到的浆料进行喷雾造粒,得到球形料;将所述球形料依次进行第一烧结和第二烧结,得到高熵硼化物微球;以所述高熵硼化物微球为涂料,在基体上进行喷涂,得到所述高熵硼化物涂层。本发明得到的高熵硼化物涂层具有较高的致密性。
Preparation method of high-entropy boride coating
The invention belongs to the technical field of high-entropy borides, and particularly relates to a preparation method of a high-entropy boride coating. The invention provides a preparation method of a high-entropy boride coating, which comprises the following steps: mixing high-entropy boride, a dispersant and a binder, and carrying out spray granulation on the obtained slurry to obtain a spherical material; sequentially carrying out first sintering and second sintering on the spherical material to obtain the high-entropy boride microspheres, and spraying the high-entropy boride microspheres serving as a coating on a matrix to obtain the high-entropy boride coating. The high-entropy boride coating obtained by the method disclosed by the invention has relatively high compactness.
本发明属于高熵硼化物技术领域,具体涉及一种高熵硼化物涂层的制备方法。本发明提供了一种高熵硼化物涂层的制备方法,包括以下步骤:将高熵硼化物、分散剂和粘结剂混合,得到的浆料进行喷雾造粒,得到球形料;将所述球形料依次进行第一烧结和第二烧结,得到高熵硼化物微球;以所述高熵硼化物微球为涂料,在基体上进行喷涂,得到所述高熵硼化物涂层。本发明得到的高熵硼化物涂层具有较高的致密性。
Preparation method of high-entropy boride coating
一种高熵硼化物涂层的制备方法
LIU YANBO (Autor:in) / MA ZHUANG (Autor:in) / LIU LING (Autor:in) / CHI HUANYU (Autor:in) / ZHANG ZE (Autor:in) / LIU SHAOPU (Autor:in) / MOU GUANGYI (Autor:in) / HE SIYUAN (Autor:in)
05.09.2023
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
High-entropy boride coating as well as preparation method and application thereof
Europäisches Patentamt | 2024
|Silicon-containing high-entropy boride coating as well as preparation method and application thereof
Europäisches Patentamt | 2024
|Quaternary boride high-entropy ceramic and preparation method thereof
Europäisches Patentamt | 2024
|Preparation method of high-entropy boride infrared radiation material
Europäisches Patentamt | 2024
|Europäisches Patentamt | 2023
|