Preparation method of microwave modified waste rubber cement soil
The invention relates to a preparation method of microwave modified waste rubber cement soil, which comprises the following steps: placing waste rubber particles in a microwave oven for microwave modification for 10 minutes at the power of 700w to obtain modified waste rubber particles after the microwave oven power is 700w; according to the microwave modified waste rubber cement soil, the waste rubber particles are subjected to microwave modification, so that the compressive strength of the prepared microwave modified waste rubber cement soil is improved, the compressive strength of the microwave modified waste rubber cement soil is improved, and the compressive strength of the microwave modified waste rubber cement soil is improved; the method has the characteristics of simplicity, convenience in operation and the like.
本发明涉及一种微波改性废弃橡胶水泥土的制备方法,将废弃橡胶颗粒置于微波炉内微波改性,微波炉功率为700w,改性时间为10min,时间结束后即可得到改性废弃橡胶颗粒,用制得的改性废弃橡胶颗粒取代普通废弃橡胶颗粒与定量的水泥、土和水拌和均匀,得到微波改性废弃橡胶水泥土,本发明通过对废弃橡胶颗粒进行微波改性,使制备得到的微波改性废弃橡胶水泥土抗压强度提升,具有方法简单、操作方便等特点。
Preparation method of microwave modified waste rubber cement soil
The invention relates to a preparation method of microwave modified waste rubber cement soil, which comprises the following steps: placing waste rubber particles in a microwave oven for microwave modification for 10 minutes at the power of 700w to obtain modified waste rubber particles after the microwave oven power is 700w; according to the microwave modified waste rubber cement soil, the waste rubber particles are subjected to microwave modification, so that the compressive strength of the prepared microwave modified waste rubber cement soil is improved, the compressive strength of the microwave modified waste rubber cement soil is improved, and the compressive strength of the microwave modified waste rubber cement soil is improved; the method has the characteristics of simplicity, convenience in operation and the like.
本发明涉及一种微波改性废弃橡胶水泥土的制备方法,将废弃橡胶颗粒置于微波炉内微波改性,微波炉功率为700w,改性时间为10min,时间结束后即可得到改性废弃橡胶颗粒,用制得的改性废弃橡胶颗粒取代普通废弃橡胶颗粒与定量的水泥、土和水拌和均匀,得到微波改性废弃橡胶水泥土,本发明通过对废弃橡胶颗粒进行微波改性,使制备得到的微波改性废弃橡胶水泥土抗压强度提升,具有方法简单、操作方便等特点。
Preparation method of microwave modified waste rubber cement soil
一种微波改性废弃橡胶水泥土的制备方法
MA DONGDONG (Autor:in) / YUAN JIAMING (Autor:in) / JIANG DALIN (Autor:in) / DING JINMENG (Autor:in) / YU KAIYUAN (Autor:in) / LI YINHUI (Autor:in)
02.07.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Preparation method of vacuum heating modified waste rubber cement soil
Europäisches Patentamt | 2024
|Preparation method of waste rubber metakaolin cement soil
Europäisches Patentamt | 2023
|Modified waste rubber, preparation method thereof and cement-based composite material
Europäisches Patentamt | 2023
|Europäisches Patentamt | 2024
|Europäisches Patentamt | 2022
|