Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
High-crack-resistance wear-resistant self-leveling mortar
The invention discloses high-crack-resistance wear-resistant self-leveling mortar, which is prepared from the following raw materials in percentage by weight: 15 to 25 weight percent of crack-resistance Portland cement clinker, 5 to 10 weight percent of auxiliary cementing material, 3 to 7 weight percent of gypsum, 5 to 10 weight percent of heavy calcium powder, 3 to 7 weight percent of modified steel slag powder, 30 to 35 weight percent of 40 to 70-mesh quartz sand and 20 to 25 weight percent of 70 to 120-mesh quartz sand, the auxiliary materials account for the total mass percentage of the raw materials: 0.1-0.8 wt% of redispersible latex powder, 0.2-0.4 wt% of a powdery polycarboxylic acid water reducing agent, 0.01-0.02 wt% of cellulose ether and 0.1 wt% of a defoaming agent. The crack resistance and wear resistance of the self-leveling mortar are improved.
本发明公开了一种高抗裂耐磨自流平砂浆,包括重量百分比的原材料:15~25wt%抗裂硅酸盐水泥熟料、5~10wt%辅助胶凝材料、3~7wt%石膏、5~10wt%重钙粉、3~7wt%改性钢渣粉、30~35wt%40~70目石英砂、20~25wt%70~120目石英砂,以及占原材料总质量百分比的辅料:0.1~0.8wt%可再分散乳胶粉、0.2~0.4wt%粉状聚羧酸减水剂、0.01~0.02wt%纤维素醚、0.1wt%消泡剂。本发明提高了自流平砂浆抗裂性和耐磨性。
High-crack-resistance wear-resistant self-leveling mortar
The invention discloses high-crack-resistance wear-resistant self-leveling mortar, which is prepared from the following raw materials in percentage by weight: 15 to 25 weight percent of crack-resistance Portland cement clinker, 5 to 10 weight percent of auxiliary cementing material, 3 to 7 weight percent of gypsum, 5 to 10 weight percent of heavy calcium powder, 3 to 7 weight percent of modified steel slag powder, 30 to 35 weight percent of 40 to 70-mesh quartz sand and 20 to 25 weight percent of 70 to 120-mesh quartz sand, the auxiliary materials account for the total mass percentage of the raw materials: 0.1-0.8 wt% of redispersible latex powder, 0.2-0.4 wt% of a powdery polycarboxylic acid water reducing agent, 0.01-0.02 wt% of cellulose ether and 0.1 wt% of a defoaming agent. The crack resistance and wear resistance of the self-leveling mortar are improved.
本发明公开了一种高抗裂耐磨自流平砂浆,包括重量百分比的原材料:15~25wt%抗裂硅酸盐水泥熟料、5~10wt%辅助胶凝材料、3~7wt%石膏、5~10wt%重钙粉、3~7wt%改性钢渣粉、30~35wt%40~70目石英砂、20~25wt%70~120目石英砂,以及占原材料总质量百分比的辅料:0.1~0.8wt%可再分散乳胶粉、0.2~0.4wt%粉状聚羧酸减水剂、0.01~0.02wt%纤维素醚、0.1wt%消泡剂。本发明提高了自流平砂浆抗裂性和耐磨性。
High-crack-resistance wear-resistant self-leveling mortar
一种高抗裂耐磨自流平砂浆
CHONG NA (Autor:in) / XIA YANQING (Autor:in) / ZHANG YUQING (Autor:in) / ZHANG SHUIJIAN (Autor:in)
22.11.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2021
|Surface wear-resistant hydrophobic enhanced self-leveling mortar
Europäisches Patentamt | 2020
|Low-cost high-temperature-resistant self-leveling mortar
Europäisches Patentamt | 2020
|High-wear-resistance gypsum-based self-leveling mortar and preparation method thereof
Europäisches Patentamt | 2021
|