A component of a solid oxide fuel cell includes an electrolyte having a stabilized zirconia and one or more dopants. The stabilized zirconia particles can have a d50 particle size of at least 150 nm. The electrolyte can have a peak sintering temperature of not greater than 1120° C. The solid oxide fuel cell can have an average open cell voltage (OCV) of not greater than 1.09 V.
A component of a solid oxide fuel cell includes an electrolyte having a stabilized zirconia and one or more dopants. The stabilized zirconia particles can have a d50 particle size of at least 150 nm. The electrolyte can have a peak sintering temperature of not greater than 1120° C. The solid oxide fuel cell can have an average open cell voltage (OCV) of not greater than 1.09 V.
ELECTROLYTE DOPANT SYSTEM
ELEKTROLYTDOTIERSYSTEM
SYSTÈME DE DOPANT D'ÉLECTROLYTE
MOHANRAM ARAVIND (Autor:in)
29.04.2020
Patent
Elektronische Ressource
Englisch
IPC:
H01M
Verfahren oder Mittel, z.B. Batterien, für die direkte Umwandlung von chemischer in elektrische Energie
,
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
/
C01G
Verbindungen der von den Unterklassen C01D oder C01F nicht umfassten Metalle
,
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F
/
C04B
Kalk
,
LIME
British Library Online Contents | 2008
|Dopant Electromigration in Semiconductors
British Library Online Contents | 1997
|Shallow boron dopant on silicon
British Library Online Contents | 2004
|Dopant-Related Complexes in SiC
British Library Online Contents | 2000
|