A component of a solid oxide fuel cell includes an electrolyte having a stabilized zirconia and one or more dopants. The stabilized zirconia particles can have a d50 particle size of at least 150 nm. The electrolyte can have a peak sintering temperature of not greater than 1120° C. The solid oxide fuel cell can have an average open cell voltage (OCV) of not greater than 1.09 V.
A component of a solid oxide fuel cell includes an electrolyte having a stabilized zirconia and one or more dopants. The stabilized zirconia particles can have a d50 particle size of at least 150 nm. The electrolyte can have a peak sintering temperature of not greater than 1120° C. The solid oxide fuel cell can have an average open cell voltage (OCV) of not greater than 1.09 V.
ELECTROLYTE DOPANT SYSTEM
ELEKTROLYTDOTIERSYSTEM
SYSTÈME DE DOPANT D'ÉLECTROLYTE
MOHANRAM ARAVIND (author)
2020-04-29
Patent
Electronic Resource
English
IPC:
H01M
Verfahren oder Mittel, z.B. Batterien, für die direkte Umwandlung von chemischer in elektrische Energie
,
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
/
C01G
Verbindungen der von den Unterklassen C01D oder C01F nicht umfassten Metalle
,
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F
/
C04B
Kalk
,
LIME
British Library Online Contents | 2008
|Dopant Electromigration in Semiconductors
British Library Online Contents | 1997
|Shallow boron dopant on silicon
British Library Online Contents | 2004
|Dopant-Related Complexes in SiC
British Library Online Contents | 2000
|