Effect of Withdrawal Rate on Defects of Upgraded Metallurgical Grade (UMG)- Silicon Prepared by Vacuum Directional Solidification
Effect of Withdrawal Rate on Defects of Upgraded Metallurgical Grade (UMG)- Silicon Prepared by Vacuum Directional Solidification
Effect of Withdrawal Rate on Defects of Upgraded Metallurgical Grade (UMG)- Silicon Prepared by Vacuum Directional Solidification
2013-01-01
4 pages
Article (Journal)
English
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Solar cells from upgraded metallurgical-grade silicon purified by metallurgical routes
American Institute of Physics | 2013
|Refining of metallurgical silicon by directional solidification
British Library Online Contents | 2011
|Eutectic formation during directional solidification: Effect of the withdrawal rate
British Library Online Contents | 2013
|British Library Online Contents | 2011
|American Institute of Physics | 2012
|