Catalytic-materail-coated microcrystal bamboo-charcoal pottery bead and preparation method thereof
A catalytic-materail-coated microcrystal bamboo-charcoal pottery bead is prepared by coating a microcrystal bamboo-charcoal pottery bead prepared from the following compositions in percent by weight with a catalytic material: 30-50% of bamboo charcoal powder, 30-40% of a porous nonmetal mineral powder, 20-30% of clay, and 2-5% of a binder. The preparation method of the catalytic-materail-coated microcrystal bamboo-charcoal pottery bead comprises: adding the catalytic material into a silica-gel water dispersion, stirring to form a suspension, then putting the microcrystal bamboo-charcoal pottery bead into the suspension, stirring, taking out the microcrystal bamboo-charcoal pottery bead and drying; or putting the microcrystal bamboo-charcoal pottery bead into the suspension for dipping, and taking out for drying. The photocatalysis function of the catalytic material and the extremely good adsorption of the microcrystal bamboo-charcoal pottery bead are integrated, the catalytic effect of the catalytic material is improved, and the preparation method is simple and application is convenient.
Catalytic-materail-coated microcrystal bamboo-charcoal pottery bead and preparation method thereof
A catalytic-materail-coated microcrystal bamboo-charcoal pottery bead is prepared by coating a microcrystal bamboo-charcoal pottery bead prepared from the following compositions in percent by weight with a catalytic material: 30-50% of bamboo charcoal powder, 30-40% of a porous nonmetal mineral powder, 20-30% of clay, and 2-5% of a binder. The preparation method of the catalytic-materail-coated microcrystal bamboo-charcoal pottery bead comprises: adding the catalytic material into a silica-gel water dispersion, stirring to form a suspension, then putting the microcrystal bamboo-charcoal pottery bead into the suspension, stirring, taking out the microcrystal bamboo-charcoal pottery bead and drying; or putting the microcrystal bamboo-charcoal pottery bead into the suspension for dipping, and taking out for drying. The photocatalysis function of the catalytic material and the extremely good adsorption of the microcrystal bamboo-charcoal pottery bead are integrated, the catalytic effect of the catalytic material is improved, and the preparation method is simple and application is convenient.
Catalytic-materail-coated microcrystal bamboo-charcoal pottery bead and preparation method thereof
WEI ZHONGHUA (author) / WEI YUHONG (author) / WEI DONGFANG (author)
2015-04-01
Patent
Electronic Resource
English
Novel bamboo charcoal pottery clay water purification liner and preparation method thereof
European Patent Office | 2016
|Microcrystal bead high-efficiency water-permeable composite brick and preparation method thereof
European Patent Office | 2024
|Bamboo charcoal ceramic tile and preparation method thereof
European Patent Office | 2015
|Bamboo charcoal diatom purification wallpaper and preparation method thereof
European Patent Office | 2021
|