A platform for research: civil engineering, architecture and urbanism
High strength debris aerated brick
The invention discloses a high strength debris aerated brick. The high strength debris aerated brick is made from, by weight, 18-28 parts of cement, 5-7 parts of mineral powder, 5-8 parts of fly ash, 70-75 parts of debris, 1-2 parts of calcium lignin sulphonate, 1.8-2.5 parts of a CTF concrete synergist, 0.3-0.5 parts of aluminum powder, 1-2 parts of carboxylic styrene butadiene latex, 1-2 parts of calcium sulphoaluminate, 0.2-0.3 parts of chlorinated paraffin, 20-30 parts of diatomite, 10-20 parts of bentonite, 3.5-4.8 parts of sodium gluconate and 5-13 parts of compound modified concrete particles.
High strength debris aerated brick
The invention discloses a high strength debris aerated brick. The high strength debris aerated brick is made from, by weight, 18-28 parts of cement, 5-7 parts of mineral powder, 5-8 parts of fly ash, 70-75 parts of debris, 1-2 parts of calcium lignin sulphonate, 1.8-2.5 parts of a CTF concrete synergist, 0.3-0.5 parts of aluminum powder, 1-2 parts of carboxylic styrene butadiene latex, 1-2 parts of calcium sulphoaluminate, 0.2-0.3 parts of chlorinated paraffin, 20-30 parts of diatomite, 10-20 parts of bentonite, 3.5-4.8 parts of sodium gluconate and 5-13 parts of compound modified concrete particles.
High strength debris aerated brick
WANG CHANGFU (author) / MAO DONGCHAO (author) / WANG YUTONG (author) / LIU WEI (author)
2015-12-09
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Preparation method of high-strength impermeable aerated brick
European Patent Office | 2022
|High-strength moisture-proof aerated brick and preparation method thereof
European Patent Office | 2021
|