Geopolymer chemically-bonded ceramic tile and preparation method thereof
The invention relates to a geopolymer chemically-bonded ceramic tile and a preparation method thereof. The geopolymer chemically-bonded ceramic tile is prepared from solid wastes like fly ash, filtered steel and copper slag, and industrial-grade chemical raw materials. The unburned ceramic tile is prepared from, by mass, 60 to 75% of the solid wastes, 19 to 38% of a liquid activator, 1 to 3% of a base-material additive and 1 to 3% of a compound liquid additive by procedures like mixing, sieving and granulating. Due to implementation of a firing-free process, energy conversation and consumption reduction can be realized; pollution is reduced; meanwhile, performances of the geopolymer chemically-bonded ceramic tile can reach national standards of fired ceramic tiles. The geopolymer ceramic tile does not need to introduce calcined kaolin, and after 12 to 48 hours of easy and practicable special maintenance, a ceramic bonded three-dimensional network body is rapidly formed, so the ceramic tile reaches and is superior in a part of performances to the 60-day-age level of similar geopolymer materials; limited mineral resources are not consumed; and energy consumption of calcination is avoided. The geopolymer chemically-bonded ceramic tile provided by the invention can change wastes into treasures, significantly saves energy and reduces consumption, can be used as a novel building material and has extensive application prospects.
Geopolymer chemically-bonded ceramic tile and preparation method thereof
The invention relates to a geopolymer chemically-bonded ceramic tile and a preparation method thereof. The geopolymer chemically-bonded ceramic tile is prepared from solid wastes like fly ash, filtered steel and copper slag, and industrial-grade chemical raw materials. The unburned ceramic tile is prepared from, by mass, 60 to 75% of the solid wastes, 19 to 38% of a liquid activator, 1 to 3% of a base-material additive and 1 to 3% of a compound liquid additive by procedures like mixing, sieving and granulating. Due to implementation of a firing-free process, energy conversation and consumption reduction can be realized; pollution is reduced; meanwhile, performances of the geopolymer chemically-bonded ceramic tile can reach national standards of fired ceramic tiles. The geopolymer ceramic tile does not need to introduce calcined kaolin, and after 12 to 48 hours of easy and practicable special maintenance, a ceramic bonded three-dimensional network body is rapidly formed, so the ceramic tile reaches and is superior in a part of performances to the 60-day-age level of similar geopolymer materials; limited mineral resources are not consumed; and energy consumption of calcination is avoided. The geopolymer chemically-bonded ceramic tile provided by the invention can change wastes into treasures, significantly saves energy and reduces consumption, can be used as a novel building material and has extensive application prospects.
Geopolymer chemically-bonded ceramic tile and preparation method thereof
HU HAIQUAN (author) / LAI MING (author) / CHEN CHANGQING (author) / LI YUEMING (author) / WANG ZHUMEI (author) / CHEN YUNXIA (author) / CAO CHUN E (author)
2016-01-13
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Ceramic tile dry granules, preparation method thereof, ceramic tile and preparation method thereof
European Patent Office | 2022
|Preparation process of luminous ceramic tile and luminous ceramic tile thereof
European Patent Office | 2021
|Chemically bonded ceramic environment-friendly water permeable brick and preparation method thereof
European Patent Office | 2023
|