A platform for research: civil engineering, architecture and urbanism
Manufacturing method of colorful electromagnetic shielding solid wood composite floor
The invention discloses a manufacturing method of a colorful electromagnetic shielding solid wood composite floor. The manufacturing method comprises the following steps of 1, nickel plating solutionpreparation; 2, colorized solution preparation; 3, chemical plating; 4, plating layer coloring; 5, gluing; and 6, painting. The method has advantages that technical wood is used for replacing a traditional wood veneer so that a very good protection effect is achieved on famous and precious tree species; chemical nickel plating reduces surface resistivity of a technical wood veneer, a function of shielding electromagnetic radiation is achieved, harm to human bodies caused by long-term radiation is avoided; an appearance of the colorful electromagnetic shielding technical wood veneer shows a good visual effect that multiple colors such as red, blue, yellow, purple, green and the like are uniformly doped, and individual requirements of consumers are met.
一种多彩电磁屏蔽实木复合地板的制造方法,其步骤如下:一、镀镍镀液制备;二、彩化液制备;三、化学镀;四、镀层彩化;五、胶合;六、油漆,本发明有益的效果是:本发明使用科技木代替传统木材单板,对名珍贵树种起到很好的保护作用;化学镀镍降低科技木单板的表面电阻率,起到屏蔽电磁辐射的功能,避免长期辐射给人身体带来危害;发明所述多彩电磁屏蔽科技木单板外观呈现出红、蓝、黄、紫、绿等多种色彩均匀掺杂的良好视觉效果,满足消费者的个性化需求。
Manufacturing method of colorful electromagnetic shielding solid wood composite floor
The invention discloses a manufacturing method of a colorful electromagnetic shielding solid wood composite floor. The manufacturing method comprises the following steps of 1, nickel plating solutionpreparation; 2, colorized solution preparation; 3, chemical plating; 4, plating layer coloring; 5, gluing; and 6, painting. The method has advantages that technical wood is used for replacing a traditional wood veneer so that a very good protection effect is achieved on famous and precious tree species; chemical nickel plating reduces surface resistivity of a technical wood veneer, a function of shielding electromagnetic radiation is achieved, harm to human bodies caused by long-term radiation is avoided; an appearance of the colorful electromagnetic shielding technical wood veneer shows a good visual effect that multiple colors such as red, blue, yellow, purple, green and the like are uniformly doped, and individual requirements of consumers are met.
一种多彩电磁屏蔽实木复合地板的制造方法,其步骤如下:一、镀镍镀液制备;二、彩化液制备;三、化学镀;四、镀层彩化;五、胶合;六、油漆,本发明有益的效果是:本发明使用科技木代替传统木材单板,对名珍贵树种起到很好的保护作用;化学镀镍降低科技木单板的表面电阻率,起到屏蔽电磁辐射的功能,避免长期辐射给人身体带来危害;发明所述多彩电磁屏蔽科技木单板外观呈现出红、蓝、黄、紫、绿等多种色彩均匀掺杂的良好视觉效果,满足消费者的个性化需求。
Manufacturing method of colorful electromagnetic shielding solid wood composite floor
一种多彩电磁屏蔽实木复合地板的制造方法
SHEN YUYAN (author) / WANG LIJUAN (author) / DAI WEIDE (author) / DU RONG (author) / CHEN DA (author) / FENG YUEMIN (author) / YANG FENG (author) / HU ZHIXIANG (author) / DING HU (author)
2020-04-14
Patent
Electronic Resource
Chinese
Geothermal solid wood composite floor and manufacturing method thereof
European Patent Office | 2016
|Preparation method of heating solid wood composite floor and heating solid wood composite floor
European Patent Office | 2024
|Solid wood composite stair floor and manufacturing method thereof
European Patent Office | 2020
|Manufacturing process of colorful floor tiles for urban roads
European Patent Office | 2015
|