Semi-flexible composite pavement
The invention discloses a semi-flexible composite pavement. The semi-flexible composite pavement comprises an asphalt mixture, and the asphalt mixture comprises, by mass, 10-20 parts of SBS modified asphalt, 30-60 parts of basalt coarse aggregate, 20-40 parts of a macromolecular surfactant, 5-10 parts of synthetic grease, 3-5 parts of starch glue, 10-15 parts of a humectant, 3-6 parts of limestonemineral powder, 0.2-0.3 part of triisopropanolamine, 2-4 parts of monofilament polypropylene fibers, 3 parts of lipase, 5 parts of sodium tripolyphosphate, 3 parts of butyl acrylate, 4 parts of alkylglycoside and 1-3 parts of water. The semi-flexible composite pavement disclosed by the invention adopts the asphalt mixture with high stability, high strength and high and low temperature resistance, so that the obtained semi-flexible composite pavement also has high stability and high strength.
本发明公开了一种半柔性复合路面,包括沥青混合料;所述沥青混合料按质量份数由如下组分组成:SBS改性沥青10~20份、玄武岩粗集料30~60份、20~40份高分子表面活性剂、5~10份合成油脂、3~5份淀粉胶、10~15份保湿剂、石灰岩矿粉3~6份,三异丙醇胺0.2~0.3份、单丝聚丙烯纤维2~4份、3份脂肪酶、5份三聚磷酸钠、3份丙烯酸丁酯、4份烷基糖苷以及水1~3份。本发明半柔性复合路面采用具有高稳定性、高强度和耐高低温性能的沥青混合料,从而使得到的半柔性复合路面也具有高稳定性和高强度。
Semi-flexible composite pavement
The invention discloses a semi-flexible composite pavement. The semi-flexible composite pavement comprises an asphalt mixture, and the asphalt mixture comprises, by mass, 10-20 parts of SBS modified asphalt, 30-60 parts of basalt coarse aggregate, 20-40 parts of a macromolecular surfactant, 5-10 parts of synthetic grease, 3-5 parts of starch glue, 10-15 parts of a humectant, 3-6 parts of limestonemineral powder, 0.2-0.3 part of triisopropanolamine, 2-4 parts of monofilament polypropylene fibers, 3 parts of lipase, 5 parts of sodium tripolyphosphate, 3 parts of butyl acrylate, 4 parts of alkylglycoside and 1-3 parts of water. The semi-flexible composite pavement disclosed by the invention adopts the asphalt mixture with high stability, high strength and high and low temperature resistance, so that the obtained semi-flexible composite pavement also has high stability and high strength.
本发明公开了一种半柔性复合路面,包括沥青混合料;所述沥青混合料按质量份数由如下组分组成:SBS改性沥青10~20份、玄武岩粗集料30~60份、20~40份高分子表面活性剂、5~10份合成油脂、3~5份淀粉胶、10~15份保湿剂、石灰岩矿粉3~6份,三异丙醇胺0.2~0.3份、单丝聚丙烯纤维2~4份、3份脂肪酶、5份三聚磷酸钠、3份丙烯酸丁酯、4份烷基糖苷以及水1~3份。本发明半柔性复合路面采用具有高稳定性、高强度和耐高低温性能的沥青混合料,从而使得到的半柔性复合路面也具有高稳定性和高强度。
Semi-flexible composite pavement
一种半柔性复合路面
WEI TANGZHONG (author) / LI PEINING (author) / XIA XINJIE (author) / LU WANHUA (author)
2020-04-21
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2019
|INJECTION MATERIAL FOR SEMI-FLEXIBLE PAVEMENT, AND INJECTION MILK FOR SEMI-FLEXIBLE PAVEMENT
European Patent Office | 2019
|Filling type semi-flexible anti-rutting composite pavement structure
European Patent Office | 2023
|