Composite early-strength water reducing agent and preparation method and application thereof
The invention relates to the technical field of concrete admixtures, and relates to a composite early-strength water reducing agent and a preparation method and application thereof. The composite early-strength water reducing agent comprises the following components in parts by mass: 80 to 90 parts of deionized water, 60 to 70 parts of polycarboxylate-type water reducing agent, 30 to 35 parts of starch, 10 to 25 parts of fly ash, 5 to 10 parts of triethanolamine, 3 to 6 parts of defoaming agent and 1 to 4 parts of accelerator. The polycarboxylate-type water reducing agent is a mixture composedof an APEG-type water reducing agent and an MPEG-type water reducing agent in the mass ratio of (1.2-1.4): (1.3-1.6). The preparation method comprises the following steps: S1, mixing and stirring deionized water and the polycarboxylate-type water reducing agent to obtain a mixture A; S2, adding starch, fly ash and triethanolamine into the mixture A to obtain a mixture B; S3, adding a defoaming agent and an accelerator into the mixture B, and stirring to obtain the composite early-strength water reducing agent; the composite early-strength water reducing agent can be doped into cement concrete, and the effect of improving the early strength of the concrete can be improved.
本发明涉及混凝土外加剂技术领域,它涉及一种复合早强减水剂及其制备方法和应用,包括以下组分及质量份:去离子水80‑90份、聚羧酸系减水剂60‑70份、淀粉30‑35份、粉煤灰10‑25份、三乙醇胺5‑10份、消泡剂3‑6份和速凝剂1‑4份,聚羧酸系减水剂是由APEG型减水剂和MPEG型减水剂以质量比(1.2‑1.4):(1.3‑1.6)组成的混合物;制备步骤:S1、将去离子水与聚羧酸系减水剂混合搅拌得到混合物A;S2、往混合物A添加淀粉、粉煤灰和三乙醇胺得混合物B;S3、往混合物B添加消泡剂和速凝剂,搅拌得复合早强减水剂;复合早强减水剂能掺入水泥混凝土中,能提高对混凝土早期强度的提升作用。
Composite early-strength water reducing agent and preparation method and application thereof
The invention relates to the technical field of concrete admixtures, and relates to a composite early-strength water reducing agent and a preparation method and application thereof. The composite early-strength water reducing agent comprises the following components in parts by mass: 80 to 90 parts of deionized water, 60 to 70 parts of polycarboxylate-type water reducing agent, 30 to 35 parts of starch, 10 to 25 parts of fly ash, 5 to 10 parts of triethanolamine, 3 to 6 parts of defoaming agent and 1 to 4 parts of accelerator. The polycarboxylate-type water reducing agent is a mixture composedof an APEG-type water reducing agent and an MPEG-type water reducing agent in the mass ratio of (1.2-1.4): (1.3-1.6). The preparation method comprises the following steps: S1, mixing and stirring deionized water and the polycarboxylate-type water reducing agent to obtain a mixture A; S2, adding starch, fly ash and triethanolamine into the mixture A to obtain a mixture B; S3, adding a defoaming agent and an accelerator into the mixture B, and stirring to obtain the composite early-strength water reducing agent; the composite early-strength water reducing agent can be doped into cement concrete, and the effect of improving the early strength of the concrete can be improved.
本发明涉及混凝土外加剂技术领域,它涉及一种复合早强减水剂及其制备方法和应用,包括以下组分及质量份:去离子水80‑90份、聚羧酸系减水剂60‑70份、淀粉30‑35份、粉煤灰10‑25份、三乙醇胺5‑10份、消泡剂3‑6份和速凝剂1‑4份,聚羧酸系减水剂是由APEG型减水剂和MPEG型减水剂以质量比(1.2‑1.4):(1.3‑1.6)组成的混合物;制备步骤:S1、将去离子水与聚羧酸系减水剂混合搅拌得到混合物A;S2、往混合物A添加淀粉、粉煤灰和三乙醇胺得混合物B;S3、往混合物B添加消泡剂和速凝剂,搅拌得复合早强减水剂;复合早强减水剂能掺入水泥混凝土中,能提高对混凝土早期强度的提升作用。
Composite early-strength water reducing agent and preparation method and application thereof
一种复合早强减水剂及其制备方法和应用
PANG YONGXIAN (author) / PANG SENLIN (author) / YI GANGZHAO (author)
2020-06-19
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Environment-friendly composite early-strength water reducing agent and preparation method thereof
European Patent Office | 2020
|Early-strength water reducing agent and preparation method thereof
European Patent Office | 2020
|Early-strength water reducing agent and preparation method thereof
European Patent Office | 2023
|Early-strength type water reducing agent and preparation method thereof
European Patent Office | 2021
|Viscosity-reducing early-strength concrete water reducing agent and preparation method thereof
European Patent Office | 2020
|