A platform for research: civil engineering, architecture and urbanism
Low-dosage high-early-strength alkali-free liquid accelerator and preparation method thereof
The invention discloses a low-dosage high-early-strength alkali-free liquid accelerator and a preparation method thereof. The alkali-free liquid accelerator is prepared from the following raw materials: 1, an alkali-free liquid accelerator; 50%-60% of modified aluminum sulfate, 2%-4% of a fluorine-aluminum complex solution, 3%-6% of an organic cosolvent, 1%-2% of a pH regulator, 0.5%-1.5% of an inorganic stabilizer, 0.3%-0.5% of a viscosity regulator, 4%-6% of a composite early strength agent and the balance of water, wherein the sum of the mass percentages of the components is 100%. The invention also provides a preparation method of the alkali-free liquid accelerator. The preparation process of the alkali-free liquid accelerator is simple; hydrofluoric acid-free process, alkali-free, chlorine-free, rust-free steel bar, non-polluting environment. Meanwhile, when the mixing amount of the alkali-free liquid accelerator is 5%-6%, the technical requirements of GB/T35159-2017 on the alkali-free accelerator can be met, the one-day compressive strength is larger than or equal to 13.0 MPa, and the alkali-free liquid accelerator has the advantages of being low in mixing amount, good in stability, high in early strength and large in later strength retention rate.
一种低掺量高早强型无碱液体速凝剂及其制备方法,无碱液体速凝剂是由下述原料制成的:改性硫酸铝50%~60%,氟铝络合物溶液2%~4%,有机助溶剂3%~6%,pH调节剂1%~2%,无机稳定剂0.5%~1.5%,粘度调节剂0.3%~0.5%,复合早强剂4%~6%,余量为水,上述各组分的质量百分比之和为100%。本发明还提供了所述无碱液体速凝剂的制备方法。该无碱液体速凝剂制备工艺简单,不含氢氟酸,无碱、无氯,不锈蚀钢筋,不污染环境,不伤害作业人员的身体,同时该无碱液体速凝剂掺量为5%~6%时即能满足GB/T35159‑2017对无碱速凝剂的技术要求,1天抗压强度≥13.0MPa,具有掺量低、稳定性好、早期强度高、后期强度保留率大的特点。
Low-dosage high-early-strength alkali-free liquid accelerator and preparation method thereof
The invention discloses a low-dosage high-early-strength alkali-free liquid accelerator and a preparation method thereof. The alkali-free liquid accelerator is prepared from the following raw materials: 1, an alkali-free liquid accelerator; 50%-60% of modified aluminum sulfate, 2%-4% of a fluorine-aluminum complex solution, 3%-6% of an organic cosolvent, 1%-2% of a pH regulator, 0.5%-1.5% of an inorganic stabilizer, 0.3%-0.5% of a viscosity regulator, 4%-6% of a composite early strength agent and the balance of water, wherein the sum of the mass percentages of the components is 100%. The invention also provides a preparation method of the alkali-free liquid accelerator. The preparation process of the alkali-free liquid accelerator is simple; hydrofluoric acid-free process, alkali-free, chlorine-free, rust-free steel bar, non-polluting environment. Meanwhile, when the mixing amount of the alkali-free liquid accelerator is 5%-6%, the technical requirements of GB/T35159-2017 on the alkali-free accelerator can be met, the one-day compressive strength is larger than or equal to 13.0 MPa, and the alkali-free liquid accelerator has the advantages of being low in mixing amount, good in stability, high in early strength and large in later strength retention rate.
一种低掺量高早强型无碱液体速凝剂及其制备方法,无碱液体速凝剂是由下述原料制成的:改性硫酸铝50%~60%,氟铝络合物溶液2%~4%,有机助溶剂3%~6%,pH调节剂1%~2%,无机稳定剂0.5%~1.5%,粘度调节剂0.3%~0.5%,复合早强剂4%~6%,余量为水,上述各组分的质量百分比之和为100%。本发明还提供了所述无碱液体速凝剂的制备方法。该无碱液体速凝剂制备工艺简单,不含氢氟酸,无碱、无氯,不锈蚀钢筋,不污染环境,不伤害作业人员的身体,同时该无碱液体速凝剂掺量为5%~6%时即能满足GB/T35159‑2017对无碱速凝剂的技术要求,1天抗压强度≥13.0MPa,具有掺量低、稳定性好、早期强度高、后期强度保留率大的特点。
Low-dosage high-early-strength alkali-free liquid accelerator and preparation method thereof
一种低掺量高早强型无碱液体速凝剂及其制备方法
ZHAO MINGMIN (author) / WANG YONGMEI (author) / LIU ZHAOYANG (author) / DONG SHUQIANG (author) / WANG JINCHUN (author) / ZHOU HAICHENG (author) / LIU CUIFEN (author)
2020-06-26
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
High-early-strength alkali-free liquid accelerator and preparation method thereof
European Patent Office | 2021
|High-strength alkali-free liquid accelerator and preparation method thereof
European Patent Office | 2021
|High-early-strength alkali-free liquid accelerator and preparation method and formula thereof
European Patent Office | 2022
|Preparation method of early-strength high-efficiency alkali-free accelerator
European Patent Office | 2020
|Early-strength environment-friendly alkali-free accelerator and preparation method thereof
European Patent Office | 2024
|