The invention discloses a steam pressurized concrete block and a preparation method thereof, and relates to the technical field of concrete. The steam pressurized concrete block is characterized by comprising the following components in parts by weight: 50-80 parts of carbonized rice hull powder; 10 to 15 parts of quick lime; 12 to 18 parts of cement; 65 to 75 parts of fly ash; 2-8 parts of desulfurized gypsum; 0.05 to 0.15 part of aluminum powder; 0.1 to 0.15 part of sodium hydroxide; and 90-120 parts of water. The mass strength of the steam-pressurized concrete block prepared by adopting theformula is superior to that of a traditional steam-pressurized concrete block, and the steam-pressurized concrete block utilizes wastes and is more environment-friendly.
本发明公开了一种蒸汽加压混凝土砌块及其制备方法,涉及混凝土技术领域。其技术要点是:一种蒸汽加压混凝土砌块,包括如下重量份数的组分:碳化稻壳粉:50‑80份;生石灰:10‑15份;水泥:12‑18份;粉煤灰:65‑75份;脱硫石膏:2‑8份;铝粉:0.05‑0.15份;氢氧化钠:0.1‑0.15份;水:90‑120份,通过采用上述配方制备得到的蒸汽加压混凝土砌块,其质量强度均优于传统蒸汽加压混凝土砌块,且本发明进行废物利用,更加环保。
Steam pressurized concrete block and preparation method thereof
The invention discloses a steam pressurized concrete block and a preparation method thereof, and relates to the technical field of concrete. The steam pressurized concrete block is characterized by comprising the following components in parts by weight: 50-80 parts of carbonized rice hull powder; 10 to 15 parts of quick lime; 12 to 18 parts of cement; 65 to 75 parts of fly ash; 2-8 parts of desulfurized gypsum; 0.05 to 0.15 part of aluminum powder; 0.1 to 0.15 part of sodium hydroxide; and 90-120 parts of water. The mass strength of the steam-pressurized concrete block prepared by adopting theformula is superior to that of a traditional steam-pressurized concrete block, and the steam-pressurized concrete block utilizes wastes and is more environment-friendly.
本发明公开了一种蒸汽加压混凝土砌块及其制备方法,涉及混凝土技术领域。其技术要点是:一种蒸汽加压混凝土砌块,包括如下重量份数的组分:碳化稻壳粉:50‑80份;生石灰:10‑15份;水泥:12‑18份;粉煤灰:65‑75份;脱硫石膏:2‑8份;铝粉:0.05‑0.15份;氢氧化钠:0.1‑0.15份;水:90‑120份,通过采用上述配方制备得到的蒸汽加压混凝土砌块,其质量强度均优于传统蒸汽加压混凝土砌块,且本发明进行废物利用,更加环保。
Steam pressurized concrete block and preparation method thereof
一种蒸汽加压混凝土砌块及其制备方法
CHEN TINGTING (author)
2020-07-10
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
High-recycling steam pressurized concrete block and preparation method thereof
European Patent Office | 2016
|Steam pressurized concrete block and production method thereof
European Patent Office | 2023
|Steam pressurized concrete block wall and construction method thereof
European Patent Office | 2020
|