Early-strength water reducing agent for recycled aggregate concrete and preparation method thereof
The invention discloses an early-strength water reducing agent for recycled aggregate concrete and a preparation method thereof, and relates to the technical field of building materials, and every 100parts by weight of the early-strength water reducing agent for the recycled aggregate concrete comprises the following components in parts by weight: kettle bottom materials: 33-37.5 parts of water and 33-37.5 parts of polyether macromonomer; the liquid A is prepared from 3.1 to 3.4 parts of water, 3.1 to 3.4 parts of unsaturated carboxylic acid and 0.1 to 0.4 part of sodium methallyl sulfonate;liquid B: 0.04 to 0.07 part of vitamin C, 0.14 to 0.17 part of a chain transfer agent and 10 to 13 parts of water; a liquid C: 0.4 to 0.7 part of water and 0.13 to 0.16 part of an initiator; 0.3-0.6 part of caustic soda flakes, 0.3-0.45 part of a modifier and the balance of water. The early-strength water reducing agent for recycled aggregate concrete has the advantages that the setting time is shortened, the early strength is improved, the water-cement ratio is reduced, and the freeze-thaw resistance effect of concrete is improved.
本发明公开了一种再生骨料混凝土用早强减水剂及其制备方法,涉及建筑材料技术领域,再生骨料混凝土用早强减水剂,每100重量份早强减水剂包括以下重量份的组分:釜底料:水33‑37.5份、聚醚大单体33‑37.5份;A液:水3.1‑3.4份、不饱和羧酸3.1‑3.4份、甲基丙烯磺酸钠0.1‑0.4份;B液:维生素C 0.04‑0.07份、链转移剂0.14‑0.17份、水10‑13份;C液:水0.4‑0.7份、引发剂0.13‑0.16份;片碱0.3‑0.6份、0.3‑0.45份改性剂、余量为水。本发明的再生骨料混凝土用早强减水剂具有缩短凝结时间,增加早期强度,降低水灰比,增大混凝土的抗冻融效果的优点。
Early-strength water reducing agent for recycled aggregate concrete and preparation method thereof
The invention discloses an early-strength water reducing agent for recycled aggregate concrete and a preparation method thereof, and relates to the technical field of building materials, and every 100parts by weight of the early-strength water reducing agent for the recycled aggregate concrete comprises the following components in parts by weight: kettle bottom materials: 33-37.5 parts of water and 33-37.5 parts of polyether macromonomer; the liquid A is prepared from 3.1 to 3.4 parts of water, 3.1 to 3.4 parts of unsaturated carboxylic acid and 0.1 to 0.4 part of sodium methallyl sulfonate;liquid B: 0.04 to 0.07 part of vitamin C, 0.14 to 0.17 part of a chain transfer agent and 10 to 13 parts of water; a liquid C: 0.4 to 0.7 part of water and 0.13 to 0.16 part of an initiator; 0.3-0.6 part of caustic soda flakes, 0.3-0.45 part of a modifier and the balance of water. The early-strength water reducing agent for recycled aggregate concrete has the advantages that the setting time is shortened, the early strength is improved, the water-cement ratio is reduced, and the freeze-thaw resistance effect of concrete is improved.
本发明公开了一种再生骨料混凝土用早强减水剂及其制备方法,涉及建筑材料技术领域,再生骨料混凝土用早强减水剂,每100重量份早强减水剂包括以下重量份的组分:釜底料:水33‑37.5份、聚醚大单体33‑37.5份;A液:水3.1‑3.4份、不饱和羧酸3.1‑3.4份、甲基丙烯磺酸钠0.1‑0.4份;B液:维生素C 0.04‑0.07份、链转移剂0.14‑0.17份、水10‑13份;C液:水0.4‑0.7份、引发剂0.13‑0.16份;片碱0.3‑0.6份、0.3‑0.45份改性剂、余量为水。本发明的再生骨料混凝土用早强减水剂具有缩短凝结时间,增加早期强度,降低水灰比,增大混凝土的抗冻融效果的优点。
Early-strength water reducing agent for recycled aggregate concrete and preparation method thereof
一种再生骨料混凝土用早强减水剂及其制备方法
PANG YONGXIAN (author) / PANG SENLIN (author) / YI GANGZHAO (author)
2020-07-17
Patent
Electronic Resource
Chinese
Recycled aggregate reinforcing agent and preparation method thereof, and recycled aggregate concrete
European Patent Office | 2020
|European Patent Office | 2024
|European Patent Office | 2024
|High-strength recycled aggregate concrete and preparation method thereof
European Patent Office | 2023
|High-strength recycled aggregate concrete and preparation method thereof
European Patent Office | 2022
|