Coke oven burner grouting material and manufacturing method thereof
The invention discloses a coke oven burner grouting material. The coke oven burner grouting material comprises the following effective components: liquid phenolic resin serving as a base material, silicon dioxide powder, mullite powder and clay refractory mortar serving as fillers, and a silane coupling agent and polydimethylsiloxane serving as additives, wherein the mass part ratio of the base material to the fillers to the additives is (0.25-0.35): (0.64-0.74): (0.005-0.015). In addition, the invention further discloses a coke oven burner grouting material which comprises the following components in percentage by mass: 25-35% of liquid phenolic resin serving as a base material, 64-74% of silica powder, mullite powder and clay refractory mortar serving as fillers, and 0.5-1.5% of a silanecoupling agent and polydimethylsiloxane which are used as additives. In addition, the invention further discloses a manufacturing method of the coke oven burner grouting material. The coke oven burner grouting material has the characteristics of favorable flowability and favorable dispersity.
本发明公开了一种焦炉炉头灌浆料,其包括有效成分:作为基体材料的液态酚醛树脂;作为填料的二氧化硅粉、莫来粉和粘土耐火泥;作为添加剂的硅烷偶联剂和聚二甲基硅氧烷;其中以质量份数计量,基体材料:填料:添加剂为(0.25‑0.35):(0.64‑0.74):(0.005‑0.015)。此外,本发明还公开了一种焦炉炉头灌浆料,其各组分质量百分配比为:作为基体材料的液态酚醛树脂:25‑35%;作为填料的二氧化硅粉、莫来粉和粘土耐火泥:64‑74%;作为添加剂的硅烷偶联剂和聚二甲基硅氧烷:0.5‑1.5%。另外,本发明还公开了上述的焦炉炉头灌浆料的制造方法。该焦炉炉头灌浆料具有良好的流动性和分散性好的特点。
Coke oven burner grouting material and manufacturing method thereof
The invention discloses a coke oven burner grouting material. The coke oven burner grouting material comprises the following effective components: liquid phenolic resin serving as a base material, silicon dioxide powder, mullite powder and clay refractory mortar serving as fillers, and a silane coupling agent and polydimethylsiloxane serving as additives, wherein the mass part ratio of the base material to the fillers to the additives is (0.25-0.35): (0.64-0.74): (0.005-0.015). In addition, the invention further discloses a coke oven burner grouting material which comprises the following components in percentage by mass: 25-35% of liquid phenolic resin serving as a base material, 64-74% of silica powder, mullite powder and clay refractory mortar serving as fillers, and 0.5-1.5% of a silanecoupling agent and polydimethylsiloxane which are used as additives. In addition, the invention further discloses a manufacturing method of the coke oven burner grouting material. The coke oven burner grouting material has the characteristics of favorable flowability and favorable dispersity.
本发明公开了一种焦炉炉头灌浆料,其包括有效成分:作为基体材料的液态酚醛树脂;作为填料的二氧化硅粉、莫来粉和粘土耐火泥;作为添加剂的硅烷偶联剂和聚二甲基硅氧烷;其中以质量份数计量,基体材料:填料:添加剂为(0.25‑0.35):(0.64‑0.74):(0.005‑0.015)。此外,本发明还公开了一种焦炉炉头灌浆料,其各组分质量百分配比为:作为基体材料的液态酚醛树脂:25‑35%;作为填料的二氧化硅粉、莫来粉和粘土耐火泥:64‑74%;作为添加剂的硅烷偶联剂和聚二甲基硅氧烷:0.5‑1.5%。另外,本发明还公开了上述的焦炉炉头灌浆料的制造方法。该焦炉炉头灌浆料具有良好的流动性和分散性好的特点。
Coke oven burner grouting material and manufacturing method thereof
一种焦炉炉头灌浆料及其制造方法
CAO YINPING (author) / XU YONGYUE (author) / MIAO WEILIANG (author) / YU GUOPU (author) / NI SHENGQI (author)
2020-08-04
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Grouting permeation sealing method for coke oven brick gas passage
European Patent Office | 2024
|Coke oven repairing material and preparation method thereof
European Patent Office | 2024
|MORTAR, COKE OVEN UPPER STRUCTURE, AND METHOD FOR MANUFACTURING COKE OVEN UPPER STRUCTURE
European Patent Office | 2020
|COKE OVEN TEMPORARY SUPERSTRUCTURE AND CONSTRUCTION METHOD OF COKE OVEN
European Patent Office | 2015
|