A platform for research: civil engineering, architecture and urbanism
Waterproof and fireproof aerated brick and preparation method thereof
The invention discloses a waterproof and fireproof aerated brick and a preparation method thereof. The aerated brick is prepared from the following raw materials in parts by weight: 15-20 parts of cast iron slag, 10-15 parts of blast furnace slag, 8-12 parts of fly ash, 5-7 parts of natural asphalt, 8-9 parts of ceramic soil, 8-11 parts of cement, 8-12 parts of glass wool, 4-6 parts of gypsum, 1-3parts of carbon powder and a proper amount of water. The preparation method mainly comprises the following steps: (1) raw material treatment, (2) pouring, (3) standing, (4) steam curing and (5) standing. The waterproof performance and the corrosion resistance of the aerated brick are improved by using the natural asphalt, and the fireproof performance, the heat preservation performance and the sound insulation performance of the aerated brick are enhanced by using the glass wool, so that the use value of the aerated brick is improved on the whole, and the requirements of modern people are met.
本发明公开了一种防水防火加气砖及其制备方法,该加气砖由下列重量份的原料制成:铸铁矿渣15‑20份、高炉矿渣10‑15份、粉煤灰8‑12份、天然沥青5‑7份、陶瓷土8‑9份、水泥8‑11份、玻璃棉8‑12份、石膏4‑6份、炭粉1‑3份、水适量。其制备方法主要包括以下步骤:(1)原料处理、(2)浇注、(3)静养、(4)蒸养、(5)静置。本发明通过使用天然沥青提高了加气砖的防水性能和防腐性能,通过使用玻璃棉增强了加气砖的防火性能和保温、隔音性能,从而在整体上提高了加气砖的使用价值,满足现代人们的需要。
Waterproof and fireproof aerated brick and preparation method thereof
The invention discloses a waterproof and fireproof aerated brick and a preparation method thereof. The aerated brick is prepared from the following raw materials in parts by weight: 15-20 parts of cast iron slag, 10-15 parts of blast furnace slag, 8-12 parts of fly ash, 5-7 parts of natural asphalt, 8-9 parts of ceramic soil, 8-11 parts of cement, 8-12 parts of glass wool, 4-6 parts of gypsum, 1-3parts of carbon powder and a proper amount of water. The preparation method mainly comprises the following steps: (1) raw material treatment, (2) pouring, (3) standing, (4) steam curing and (5) standing. The waterproof performance and the corrosion resistance of the aerated brick are improved by using the natural asphalt, and the fireproof performance, the heat preservation performance and the sound insulation performance of the aerated brick are enhanced by using the glass wool, so that the use value of the aerated brick is improved on the whole, and the requirements of modern people are met.
本发明公开了一种防水防火加气砖及其制备方法,该加气砖由下列重量份的原料制成:铸铁矿渣15‑20份、高炉矿渣10‑15份、粉煤灰8‑12份、天然沥青5‑7份、陶瓷土8‑9份、水泥8‑11份、玻璃棉8‑12份、石膏4‑6份、炭粉1‑3份、水适量。其制备方法主要包括以下步骤:(1)原料处理、(2)浇注、(3)静养、(4)蒸养、(5)静置。本发明通过使用天然沥青提高了加气砖的防水性能和防腐性能,通过使用玻璃棉增强了加气砖的防火性能和保温、隔音性能,从而在整体上提高了加气砖的使用价值,满足现代人们的需要。
Waterproof and fireproof aerated brick and preparation method thereof
一种防水防火加气砖及其制备方法
TIAN WEIGANG (author)
2020-10-02
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Waterproof and corrosion-resistant aerated brick and preparation method thereof
European Patent Office | 2015
|Preparation method of aerated brick with good waterproof performance
European Patent Office | 2015
|Waterproof autoclaved aerated porcelain wall brick and production process thereof
European Patent Office | 2023
|