Environment-friendly dry vibration bonding agent
The invention belongs to the technical field of refractory material binders, and provides an environment-friendly dry vibration binding agent which comprises the following components in parts by weight: 20-40 parts of glucose, 50-75 parts of magnesium sulfate, 5-15 parts of silica fume, 10-30 parts of asphalt and 1-5 parts of aluminum sulfate. By means of the technical scheme, the problem that inthe prior art, after glucose is used as a binding agent for demolding, the lining strength is low is solved.
本发明属于耐火材料结合剂技术领域,提出了一种环保型干式振动结合剂,包括以下重量份的组分:葡萄糖20~40份,硫酸镁50~75份,微硅粉5~15份,还包括沥青10~30份,硫酸铝1~5份。通过上述技术方案,解决了现有技术中使用葡萄糖作结合剂脱模后衬体强度偏低的问题。
Environment-friendly dry vibration bonding agent
The invention belongs to the technical field of refractory material binders, and provides an environment-friendly dry vibration binding agent which comprises the following components in parts by weight: 20-40 parts of glucose, 50-75 parts of magnesium sulfate, 5-15 parts of silica fume, 10-30 parts of asphalt and 1-5 parts of aluminum sulfate. By means of the technical scheme, the problem that inthe prior art, after glucose is used as a binding agent for demolding, the lining strength is low is solved.
本发明属于耐火材料结合剂技术领域,提出了一种环保型干式振动结合剂,包括以下重量份的组分:葡萄糖20~40份,硫酸镁50~75份,微硅粉5~15份,还包括沥青10~30份,硫酸铝1~5份。通过上述技术方案,解决了现有技术中使用葡萄糖作结合剂脱模后衬体强度偏低的问题。
Environment-friendly dry vibration bonding agent
一种环保型干式振动结合剂
XING WEIJIE (author)
2020-11-20
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Environment-friendly ceramic bonding agent and preparation method thereof
European Patent Office | 2015
|European Patent Office | 2024
|