Damp-proof ceramic tile binder and preparation method thereof
The invention belongs to the technical field of ceramic tile binders, and relates to a damp-proof ceramic tile binder and a preparation method thereof. The damp-proof ceramic tile binder is prepared from the following raw materials in parts by weight: 5-15 parts of styrene-acrylic acid copolymer emulsion, 20-35 parts of vinyl acetate-acrylate-higher fatty acid copolymer emulsion, 30-40 parts of deionized water, 1-10 parts of cellulose ether, 1-4 parts of a defoaming agent, 2-6 parts of starch ether, 15-35 parts of cement, 10-20 parts of calcium formate, 5-15 parts of talcum powder, 5-15 partsof slaked lime and 20-35 parts of quartz sand, 10-20 parts of gypsum powder, 5-15 parts of kaolin, 0.2-0.6 part of a mildew preventive and 0.1-0.5 part of an anti-freezing agent. Through the styrene-acrylic acid copolymer emulsion, the vinyl acetate-acrylate-higher fatty acid copolymer emulsion, the starch ether, the slaked lime, the quartz sand, the gypsum powder, the kaolin and the mildew preventive are adopted, so that the bonding strength of the ceramic tile binder is remarkably improved, the weather resistance of the ceramic tile binder is improved, and the ceramic tile binder has damp-proof and mildew-proof properties; and the service life of the ceramic tile binder is prolonged.
本发明属于瓷砖粘结剂技术领域,尤其为一种防潮瓷砖粘结剂及其制备方法,所述防潮瓷砖粘结剂包括以下重量份的原料:苯乙烯‑丙烯酸共聚乳液5‑15份、醋酸乙烯‑丙烯酸脂‑高级脂肪酸共聚乳液20‑35份、去离子水30‑40份、纤维素醚1‑10份、消泡剂1‑4份、淀粉醚2‑6份、水泥15‑35份、甲酸钙10‑20份、滑石粉5‑15份、熟石灰5‑15份、石英砂20‑35份、石膏粉10‑20份、高岭土5‑15份、防霉剂0.2‑0.6份和防冻剂0.1‑0.5份。本发明通过苯乙烯‑丙烯酸共聚乳液、醋酸乙烯‑丙烯酸脂‑高级脂肪酸共聚乳液、淀粉醚、熟石灰、石英砂、石膏粉、高岭土和防霉剂,显著提高瓷砖粘结剂的粘结强度,提高瓷砖粘结剂的耐候性,使瓷砖粘结剂具有防潮和防霉的性能,提高瓷砖粘结剂的使用寿命。
Damp-proof ceramic tile binder and preparation method thereof
The invention belongs to the technical field of ceramic tile binders, and relates to a damp-proof ceramic tile binder and a preparation method thereof. The damp-proof ceramic tile binder is prepared from the following raw materials in parts by weight: 5-15 parts of styrene-acrylic acid copolymer emulsion, 20-35 parts of vinyl acetate-acrylate-higher fatty acid copolymer emulsion, 30-40 parts of deionized water, 1-10 parts of cellulose ether, 1-4 parts of a defoaming agent, 2-6 parts of starch ether, 15-35 parts of cement, 10-20 parts of calcium formate, 5-15 parts of talcum powder, 5-15 partsof slaked lime and 20-35 parts of quartz sand, 10-20 parts of gypsum powder, 5-15 parts of kaolin, 0.2-0.6 part of a mildew preventive and 0.1-0.5 part of an anti-freezing agent. Through the styrene-acrylic acid copolymer emulsion, the vinyl acetate-acrylate-higher fatty acid copolymer emulsion, the starch ether, the slaked lime, the quartz sand, the gypsum powder, the kaolin and the mildew preventive are adopted, so that the bonding strength of the ceramic tile binder is remarkably improved, the weather resistance of the ceramic tile binder is improved, and the ceramic tile binder has damp-proof and mildew-proof properties; and the service life of the ceramic tile binder is prolonged.
本发明属于瓷砖粘结剂技术领域,尤其为一种防潮瓷砖粘结剂及其制备方法,所述防潮瓷砖粘结剂包括以下重量份的原料:苯乙烯‑丙烯酸共聚乳液5‑15份、醋酸乙烯‑丙烯酸脂‑高级脂肪酸共聚乳液20‑35份、去离子水30‑40份、纤维素醚1‑10份、消泡剂1‑4份、淀粉醚2‑6份、水泥15‑35份、甲酸钙10‑20份、滑石粉5‑15份、熟石灰5‑15份、石英砂20‑35份、石膏粉10‑20份、高岭土5‑15份、防霉剂0.2‑0.6份和防冻剂0.1‑0.5份。本发明通过苯乙烯‑丙烯酸共聚乳液、醋酸乙烯‑丙烯酸脂‑高级脂肪酸共聚乳液、淀粉醚、熟石灰、石英砂、石膏粉、高岭土和防霉剂,显著提高瓷砖粘结剂的粘结强度,提高瓷砖粘结剂的耐候性,使瓷砖粘结剂具有防潮和防霉的性能,提高瓷砖粘结剂的使用寿命。
Damp-proof ceramic tile binder and preparation method thereof
一种防潮瓷砖粘结剂及其制备方法
ZHOU PING'AN (author) / HUANG XIAOJIN (author)
2020-12-25
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Damp-proof waterproof binder for building and preparation method of damp-proof waterproof binder
European Patent Office | 2015
|Damp-proof household storage cabinet and damp-proof method thereof
European Patent Office | 2021
SiO2f/SiO2 ceramic damp-proof sealing coating and preparation method thereof
European Patent Office | 2020
|Cement-based ceramic tile binder and preparation method thereof
European Patent Office | 2021
|