Environment-friendly cement brick and manufacturing process thereof
The invention discloses an environment-friendly cement brick and a manufacturing process thereof. The environment-friendly cement brick comprises a brick body, and the brick body is composed of the following components in parts by weight: 20-80 parts of cement; 30-50 parts of fly ash; 10-20 parts of quick lime; 80-100 parts of aggregate; 20-30 parts of mirabilite; 5-10 parts of ceramsite; and 1-5parts of an assistant. According to the present invention, the ratio is reasonable, such that the prepared cement brick has characteristics of high strength, high bearing capacity, good compression resistance and good shock resistance, and the mass of the brick body is substantially reduced so as to make the cement brick have advantages of light weight and high strength, and the production processof the environment-friendly cement brick comprises the following steps: premixing, secondary mixing, compression molding and drying, the manufacturing process is simple, the process continuity is good, the cement brick manufacturing efficiency is high, and the requirement for large-batch production is met.
本发明公开了一种环保型水泥砖及其制作工艺,包括砖体,砖体由如下重量份数的组分组成:水泥20‑80份;粉煤灰30‑50份;生石灰10‑20份;骨料80‑100份;石硝20‑30份;陶粒5‑10份;助剂1‑5份,配比合理,使得制成的水泥砖具有较高的强度和承载能力,抗压抗震性能较好,且极大地减轻了砖体的质量,使得水泥砖能够兼顾质轻和高强度的优点,环保型水泥砖的制作工艺包括如下步骤:预混料、二次混料、压制成型和晾干,制作工艺流程简单,工艺连续性好,水泥砖制作效率高,符合大批量生产的需要。
Environment-friendly cement brick and manufacturing process thereof
The invention discloses an environment-friendly cement brick and a manufacturing process thereof. The environment-friendly cement brick comprises a brick body, and the brick body is composed of the following components in parts by weight: 20-80 parts of cement; 30-50 parts of fly ash; 10-20 parts of quick lime; 80-100 parts of aggregate; 20-30 parts of mirabilite; 5-10 parts of ceramsite; and 1-5parts of an assistant. According to the present invention, the ratio is reasonable, such that the prepared cement brick has characteristics of high strength, high bearing capacity, good compression resistance and good shock resistance, and the mass of the brick body is substantially reduced so as to make the cement brick have advantages of light weight and high strength, and the production processof the environment-friendly cement brick comprises the following steps: premixing, secondary mixing, compression molding and drying, the manufacturing process is simple, the process continuity is good, the cement brick manufacturing efficiency is high, and the requirement for large-batch production is met.
本发明公开了一种环保型水泥砖及其制作工艺,包括砖体,砖体由如下重量份数的组分组成:水泥20‑80份;粉煤灰30‑50份;生石灰10‑20份;骨料80‑100份;石硝20‑30份;陶粒5‑10份;助剂1‑5份,配比合理,使得制成的水泥砖具有较高的强度和承载能力,抗压抗震性能较好,且极大地减轻了砖体的质量,使得水泥砖能够兼顾质轻和高强度的优点,环保型水泥砖的制作工艺包括如下步骤:预混料、二次混料、压制成型和晾干,制作工艺流程简单,工艺连续性好,水泥砖制作效率高,符合大批量生产的需要。
Environment-friendly cement brick and manufacturing process thereof
一种环保型水泥砖及其制作工艺
DAI JIANSONG (author)
2021-01-05
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Environment-friendly brick manufacturing process and mold
European Patent Office | 2021
|Environment-friendly brick and preparation process thereof
European Patent Office | 2020
|Environment-friendly brick and preparation process thereof
European Patent Office | 2024
|Environment-friendly brick and preparation process thereof
European Patent Office | 2020
|Environment-friendly PC brick and manufacturing method thereof
European Patent Office | 2022
|