Ratio and preparation method of inorganic mineral powder coating
The invention discloses a ratio and a preparation method of an inorganic mineral powder coating. The inorganic mineral powder coating comprises the following important components: 30%-40% of coarse whiting, 20%-30% of ash calcium, 15%-25% of attapulgite powder, 15%-25% of cellulose, 9%-19% of dispersible rubber powder and 1%-11% of a nano material. The preparation method of the inorganic mineral powder coating comprises the following steps: step 1, preparing the raw materials according to the proportion; step 2, putting the prepared raw materials into a dry powder stirrer to be fully stirred;step 3, packaging the uniformly stirred mixture; the water resistance and adsorbability of the coating are improved; the inorganic mineral powder coating is very wide in application, has all characteristics of the traditional coating, and can be directly constructed without a putty layer; the coating is environment-friendly, labor-saving and money-saving; formaldehyde and peculiar smell can be decomposed by adding the nano material; the coating is reasonable in design and worthy of vigorous popularization.
本发明公开了一种无机矿物粉末涂料的配比及其制作方法,所述无机矿物粉末涂料的重要组成成分如下所示:重钙30%‑40%,灰钙20%‑30%,凹凸棒粉15%‑25%,纤维素15%‑25%,可分散性胶粉9%‑19%,纳米材料1%‑11%;述无机矿物粉末涂料的制作方法如下所示:步骤1:按上述比例准备原料;步骤2:将准备好的原料放入干粉搅拌机中进行充分搅拌;步骤3:将搅拌均匀的混合物进行包装;本发明提高的涂料的耐水性、吸附性;无机矿物粉末涂料应用十分广泛,不但拥有传统涂料的所有特性,可不用做腻子层,直接施工;既环保又省工、省钱;纳米材料的添加可以分解甲醛和异味;本发明设计合理,值得大力推广。
Ratio and preparation method of inorganic mineral powder coating
The invention discloses a ratio and a preparation method of an inorganic mineral powder coating. The inorganic mineral powder coating comprises the following important components: 30%-40% of coarse whiting, 20%-30% of ash calcium, 15%-25% of attapulgite powder, 15%-25% of cellulose, 9%-19% of dispersible rubber powder and 1%-11% of a nano material. The preparation method of the inorganic mineral powder coating comprises the following steps: step 1, preparing the raw materials according to the proportion; step 2, putting the prepared raw materials into a dry powder stirrer to be fully stirred;step 3, packaging the uniformly stirred mixture; the water resistance and adsorbability of the coating are improved; the inorganic mineral powder coating is very wide in application, has all characteristics of the traditional coating, and can be directly constructed without a putty layer; the coating is environment-friendly, labor-saving and money-saving; formaldehyde and peculiar smell can be decomposed by adding the nano material; the coating is reasonable in design and worthy of vigorous popularization.
本发明公开了一种无机矿物粉末涂料的配比及其制作方法,所述无机矿物粉末涂料的重要组成成分如下所示:重钙30%‑40%,灰钙20%‑30%,凹凸棒粉15%‑25%,纤维素15%‑25%,可分散性胶粉9%‑19%,纳米材料1%‑11%;述无机矿物粉末涂料的制作方法如下所示:步骤1:按上述比例准备原料;步骤2:将准备好的原料放入干粉搅拌机中进行充分搅拌;步骤3:将搅拌均匀的混合物进行包装;本发明提高的涂料的耐水性、吸附性;无机矿物粉末涂料应用十分广泛,不但拥有传统涂料的所有特性,可不用做腻子层,直接施工;既环保又省工、省钱;纳米材料的添加可以分解甲醛和异味;本发明设计合理,值得大力推广。
Ratio and preparation method of inorganic mineral powder coating
一种无机矿物粉末涂料的配比及其制作方法
HAN YOUZHI (author)
2021-01-29
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2020
|Inorganic dry powder texture coating and preparation method
European Patent Office | 2015
|Water-based inorganic mineral composite terrace coating and preparation method thereof
European Patent Office | 2020
|Indoor inorganic dry powder building coating and preparation method thereof
European Patent Office | 2015
|