Utilization method of graphite tailings
The invention provides a utilization method of graphite tailings, which adopts graphite tailings, soda ash, calcium carbonate and dolomite as main raw materials and a small amount of boric acid or borax as an additive, carrying out high-temperature calcination melting in a high-temperature furnace, cooling water to form water-quenched particles, carrying out ball milling by a ball mill, and screening to obtain a low-melting-point powder assistant; the low-temperature co-fired ceramic additive can be used as a good additive of low-temperature co-fired ceramic. According to the powder additive prepared by the method, the calcining temperature of the co-fired ceramic is effectively reduced, the energy consumption is reduced, meanwhile, the graphite tailings are effectively utilized as processing raw materials, the powder additive is more environment-friendly, and efficient utilization of solid waste resources is realized.
本发明提供一种石墨尾矿的利用方法,以石墨尾矿、纯碱、碳酸钙、白云石为主要原料,以少量硼酸或硼砂作为添加剂,在高温炉中进行高温煅烧熔制,然后过冷却水后形成水淬颗粒,经球磨机球磨后筛分得到低熔点粉体助剂,可作为一种低温共烧陶瓷的良好助剂。本发明制备得到的粉体助剂有效地降低共烧陶瓷的煅烧温度,降低能耗,同时有效地利用了石墨尾矿作为加工原料,更环保,实现固废资源的高效利用。
Utilization method of graphite tailings
The invention provides a utilization method of graphite tailings, which adopts graphite tailings, soda ash, calcium carbonate and dolomite as main raw materials and a small amount of boric acid or borax as an additive, carrying out high-temperature calcination melting in a high-temperature furnace, cooling water to form water-quenched particles, carrying out ball milling by a ball mill, and screening to obtain a low-melting-point powder assistant; the low-temperature co-fired ceramic additive can be used as a good additive of low-temperature co-fired ceramic. According to the powder additive prepared by the method, the calcining temperature of the co-fired ceramic is effectively reduced, the energy consumption is reduced, meanwhile, the graphite tailings are effectively utilized as processing raw materials, the powder additive is more environment-friendly, and efficient utilization of solid waste resources is realized.
本发明提供一种石墨尾矿的利用方法,以石墨尾矿、纯碱、碳酸钙、白云石为主要原料,以少量硼酸或硼砂作为添加剂,在高温炉中进行高温煅烧熔制,然后过冷却水后形成水淬颗粒,经球磨机球磨后筛分得到低熔点粉体助剂,可作为一种低温共烧陶瓷的良好助剂。本发明制备得到的粉体助剂有效地降低共烧陶瓷的煅烧温度,降低能耗,同时有效地利用了石墨尾矿作为加工原料,更环保,实现固废资源的高效利用。
Utilization method of graphite tailings
一种石墨尾矿的利用方法
PENG SHOU (author) / REN DONGFENG (author) / WEN GUIQIANG (author) / CHEN TAO (author) / LI XINYU (author) / LI YUFENG (author) / LIU HAIDONG (author) / WANG WENQI (author)
2021-03-19
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Method for preparing light ceramic tile from graphite tailings
European Patent Office | 2020
|Bearing capacity mechanism of soilbagged graphite tailings
Springer Verlag | 2024
|Comprehensive utilization device and method for copper tailings
European Patent Office | 2022
|Method for preparing concrete underground pipe gallery from graphite tailings
European Patent Office | 2020
|Process method for preparing sintered pavement brick from graphite tailings
European Patent Office | 2024
|