Cement-based self-leveling mortar and preparation process thereof
The invention relates to the technical field of dry-mixed mortar, and particularly discloses cement-based self-leveling mortar and a preparation process thereof. The cement-based self-leveling mortar is prepared from the following components in parts by weight: 200 to 300 parts of cement, 20 to 60 parts of gypsum, 50 to 100 parts of sulphoaluminate cement, 0.5 to 1.5 parts of cellulose, 0.8 to 2.0 parts of water reducing agent, 0.5 to 1.0 part of defoaming agent, 0.2 to 0.5 part of coagulation accelerator, 0.5 to 1.2 parts of retarder, 400 to 600 parts of graded sand, 130 to 180 parts of filler, 30 to 50 parts of epoxy resin and 20 to 50 parts of bean flour. The mortar has the advantages of being good in wear resistance and not prone to generating dust.
本申请涉及干混砂浆技术领域,具体公开了一种水泥基自流平砂浆及其制备工艺。一种水泥基自流平砂浆包括200‑300份的水泥、20‑60份的石膏、50‑100份的硫铝酸盐水泥、0.5‑1.5份的纤维素、0.8‑2.0份的减水剂、0.5‑1.0份的消泡剂、0.2‑0.5份的促凝剂、0.5‑1.2份的缓凝剂、400‑600份的级配砂、130‑180份的填料、环氧树脂30‑50份、20‑50份的豆粉;本申请具有耐磨性好、不易产生粉尘的优点。
Cement-based self-leveling mortar and preparation process thereof
The invention relates to the technical field of dry-mixed mortar, and particularly discloses cement-based self-leveling mortar and a preparation process thereof. The cement-based self-leveling mortar is prepared from the following components in parts by weight: 200 to 300 parts of cement, 20 to 60 parts of gypsum, 50 to 100 parts of sulphoaluminate cement, 0.5 to 1.5 parts of cellulose, 0.8 to 2.0 parts of water reducing agent, 0.5 to 1.0 part of defoaming agent, 0.2 to 0.5 part of coagulation accelerator, 0.5 to 1.2 parts of retarder, 400 to 600 parts of graded sand, 130 to 180 parts of filler, 30 to 50 parts of epoxy resin and 20 to 50 parts of bean flour. The mortar has the advantages of being good in wear resistance and not prone to generating dust.
本申请涉及干混砂浆技术领域,具体公开了一种水泥基自流平砂浆及其制备工艺。一种水泥基自流平砂浆包括200‑300份的水泥、20‑60份的石膏、50‑100份的硫铝酸盐水泥、0.5‑1.5份的纤维素、0.8‑2.0份的减水剂、0.5‑1.0份的消泡剂、0.2‑0.5份的促凝剂、0.5‑1.2份的缓凝剂、400‑600份的级配砂、130‑180份的填料、环氧树脂30‑50份、20‑50份的豆粉;本申请具有耐磨性好、不易产生粉尘的优点。
Cement-based self-leveling mortar and preparation process thereof
一种水泥基自流平砂浆及其制备工艺
NI BIN (author) / WANG XUEPING (author) / LEI CHANGLI (author) / CUI RUKAI (author) / ZHUANG HUANHUAN (author) / XU WENHAO (author)
2021-08-06
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Cement-based self-leveling mortar and preparation method thereof
European Patent Office | 2020
|Cement-based self-leveling mortar and preparation method thereof
European Patent Office | 2020
|Cement-based self-leveling mortar and preparation method thereof
European Patent Office | 2015
|Cement-based self-leveling cushion mortar and preparation method thereof
European Patent Office | 2021
|