Mud suitable for automatic grouting line of wine bottle
The invention discloses mud suitable for an automatic grouting line of a wine bottle. The mud suitable for the automatic grouting line of the wine bottle comprises a ball milling material and a slurrying material, wherein the ball-milling material comprises ball-milling raw materials, ballstone and ball-milling water, and a ratio of the ball-milling raw material to the ballstone to the ball-milling water is 1: 1.5: 1; the ball-milling raw materials comprise, in parts by weight, 28-32 parts by weight of Yucheng potassium feldspar from Hubei Province, 16-20 parts by weight of quartz from Fengyang county, Anhu Province, 3-7 parts by weight of black clay from Zhangzhou City, Fujian Province, 0.5-5.0 parts by weight of a plasticizer and 2-5 parts by weight of dolomite; the slurrying material comprises slurrying raw materials and slurrying water, and a ratio of the slurrying raw materials to the slurrying water is 7: 3; the slurrying raw materials comprise, in parts by weight, 19-23 parts of washed kaolin from Zhangzhou City, Fujian Province, and 19-23 parts by weight of washed kaolin from Inner Mongolia. The mud suitable for the automatic grouting line of the wine bottle is suitable for production of an automatic grouting machine, good in hydrophobicity, stable and easy to adjust, and capable of reducing a pore rate and increasing an average qualification rate.
一种适宜酒瓶自动注浆线的泥浆,所述适宜酒瓶自动注浆线的泥浆包括球磨料以及化浆料;所述球磨料包括球磨原料、球石以及球磨用水,所述球磨原料、球石以及球磨用水的比例为1:1.5:1;所述球磨原料包括按重量份计的以下组分:湖北玉成钾长石28‑‑32重量份;安徽凤阳石英16‑‑20重量份;福建漳州黑泥3‑‑7重量份;增塑剂0.5‑‑5.0重量份;白云石2‑‑5重量份;所述化浆料包括化浆原料以及化浆用水,所述化浆原料以及化浆用水的比例为7:3;所述化浆原料包括按重量份计的以下组分:福建漳州水洗高岭土19‑‑23重量份;内蒙古水洗高岭土19‑‑23重量份。一种适宜酒瓶自动注浆线的泥浆,适合自动注浆机生产,疏水性好,稳定,容易调整,降低毛孔率,提高平均合格率。
Mud suitable for automatic grouting line of wine bottle
The invention discloses mud suitable for an automatic grouting line of a wine bottle. The mud suitable for the automatic grouting line of the wine bottle comprises a ball milling material and a slurrying material, wherein the ball-milling material comprises ball-milling raw materials, ballstone and ball-milling water, and a ratio of the ball-milling raw material to the ballstone to the ball-milling water is 1: 1.5: 1; the ball-milling raw materials comprise, in parts by weight, 28-32 parts by weight of Yucheng potassium feldspar from Hubei Province, 16-20 parts by weight of quartz from Fengyang county, Anhu Province, 3-7 parts by weight of black clay from Zhangzhou City, Fujian Province, 0.5-5.0 parts by weight of a plasticizer and 2-5 parts by weight of dolomite; the slurrying material comprises slurrying raw materials and slurrying water, and a ratio of the slurrying raw materials to the slurrying water is 7: 3; the slurrying raw materials comprise, in parts by weight, 19-23 parts of washed kaolin from Zhangzhou City, Fujian Province, and 19-23 parts by weight of washed kaolin from Inner Mongolia. The mud suitable for the automatic grouting line of the wine bottle is suitable for production of an automatic grouting machine, good in hydrophobicity, stable and easy to adjust, and capable of reducing a pore rate and increasing an average qualification rate.
一种适宜酒瓶自动注浆线的泥浆,所述适宜酒瓶自动注浆线的泥浆包括球磨料以及化浆料;所述球磨料包括球磨原料、球石以及球磨用水,所述球磨原料、球石以及球磨用水的比例为1:1.5:1;所述球磨原料包括按重量份计的以下组分:湖北玉成钾长石28‑‑32重量份;安徽凤阳石英16‑‑20重量份;福建漳州黑泥3‑‑7重量份;增塑剂0.5‑‑5.0重量份;白云石2‑‑5重量份;所述化浆料包括化浆原料以及化浆用水,所述化浆原料以及化浆用水的比例为7:3;所述化浆原料包括按重量份计的以下组分:福建漳州水洗高岭土19‑‑23重量份;内蒙古水洗高岭土19‑‑23重量份。一种适宜酒瓶自动注浆线的泥浆,适合自动注浆机生产,疏水性好,稳定,容易调整,降低毛孔率,提高平均合格率。
Mud suitable for automatic grouting line of wine bottle
一种适宜酒瓶自动注浆线的泥浆
XIAO SHUMING (author)
2022-02-18
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Method for preparing slurry suitable for automatic grouting line of wine bottle
European Patent Office | 2022
|Grouting device and method suitable for double-liquid grouting
European Patent Office | 2021
|Grouting system and technology suitable for high slope curtain grouting stability control
European Patent Office | 2021
|