One-glaze two-sided ceramic rock plate, one-glaze two-sided transparent glaze and preparation method thereof
The invention relates to a one-glaze two-sided ceramic rock plate, one-glaze two-sided transparent glaze and a preparation method thereof. The one-glaze two-sided ceramic rock plate sequentially comprises a green body layer, a ground glaze layer, an ink-jet decoration layer, a rubber roller printing ink protection layer and a one-glaze two-sided transparent glaze layer from bottom to top. The one-glaze two-sided transparent glaze is prepared from the following components in percentage by weight: 6.06% of lithium chinastone, 3.03% of burnt zinc oxide, 15.15% of soda powder, 7.07% of dolomite, 30.30% of DW transparent frit, 20.20% of GW transparent frit, 2.02% of barium carbonate, 3.03% of strontium carbonate, 8.09% of kaolin, 2.02% of emery powder and 3.03% of superfine quartz powder. By adjusting the proportion of the GW transparent frit and the DW transparent frit, a glaze layer which is stable in color gamut, 8-20 degrees in glossiness, good in transparency and fine and smooth in hand feeling is obtained after firing, and the polishing condition is met.
本发明涉及一釉两面陶瓷岩板、一釉两面透明釉及其制备方法。一釉两面陶瓷岩板从下到上依次包括:坯体层、底釉层、喷墨装饰层、胶辊印墨水保护层、一釉两面透明釉层。一釉两面透明釉,按重量百分比由以下组分组成:锂瓷石6.06%、烧氧化锌3.03%、钠石粉15.15%、白云石7.07%、DW透明熔块30.30%、GW透明熔块20.20%、碳酸钡2.02%、碳酸锶3.03%、高岭土8.09%、刚玉粉2.02%,超细石英粉3.03%。本发明通过GW透明熔块与DW透明熔块配比的调整,烧成后获得色域稳定、光泽度8~20度,透感好,手感细腻平滑的釉料层,满足抛光条件。
One-glaze two-sided ceramic rock plate, one-glaze two-sided transparent glaze and preparation method thereof
The invention relates to a one-glaze two-sided ceramic rock plate, one-glaze two-sided transparent glaze and a preparation method thereof. The one-glaze two-sided ceramic rock plate sequentially comprises a green body layer, a ground glaze layer, an ink-jet decoration layer, a rubber roller printing ink protection layer and a one-glaze two-sided transparent glaze layer from bottom to top. The one-glaze two-sided transparent glaze is prepared from the following components in percentage by weight: 6.06% of lithium chinastone, 3.03% of burnt zinc oxide, 15.15% of soda powder, 7.07% of dolomite, 30.30% of DW transparent frit, 20.20% of GW transparent frit, 2.02% of barium carbonate, 3.03% of strontium carbonate, 8.09% of kaolin, 2.02% of emery powder and 3.03% of superfine quartz powder. By adjusting the proportion of the GW transparent frit and the DW transparent frit, a glaze layer which is stable in color gamut, 8-20 degrees in glossiness, good in transparency and fine and smooth in hand feeling is obtained after firing, and the polishing condition is met.
本发明涉及一釉两面陶瓷岩板、一釉两面透明釉及其制备方法。一釉两面陶瓷岩板从下到上依次包括:坯体层、底釉层、喷墨装饰层、胶辊印墨水保护层、一釉两面透明釉层。一釉两面透明釉,按重量百分比由以下组分组成:锂瓷石6.06%、烧氧化锌3.03%、钠石粉15.15%、白云石7.07%、DW透明熔块30.30%、GW透明熔块20.20%、碳酸钡2.02%、碳酸锶3.03%、高岭土8.09%、刚玉粉2.02%,超细石英粉3.03%。本发明通过GW透明熔块与DW透明熔块配比的调整,烧成后获得色域稳定、光泽度8~20度,透感好,手感细腻平滑的釉料层,满足抛光条件。
One-glaze two-sided ceramic rock plate, one-glaze two-sided transparent glaze and preparation method thereof
一釉两面陶瓷岩板、一釉两面透明釉及其制备方法
PAN CHAOXIAN (author) / YANG QINGXIA (author) / DAI HUAIFANG (author) / CHE LIU (author) / LYU ZHENGPING (author)
2022-06-21
Patent
Electronic Resource
Chinese
European Patent Office | 2020
|Transparent glaze layer applied to surface of rock plate and preparation method of glaze layer
European Patent Office | 2020
|Cracked glaze, preparation method thereof and sanitary ceramic containing cracked glaze
European Patent Office | 2024
|