A platform for research: civil engineering, architecture and urbanism
Civil building anti-crack mortar and preparation method thereof
The invention relates to civil building anti-crack mortar and a preparation method thereof. The civil building anti-crack mortar is prepared from the following raw materials in parts by weight: 200 to 350 parts of Portland cement, 400 to 500 parts of machine-made sand, 100 to 200 parts of rubber particles, 50 to 80 parts of composite admixture, 2 to 3 parts of cellulose ether, 5 to 15 parts of redispersible latex powder, 0.1 to 0.3 part of starch ether and 1 to 3 parts of polypropylene fiber. According to the civil building anti-crack mortar, various components are scientifically matched, so that the civil building anti-crack mortar has good comprehensive performance and is short in setting time, high in strength, excellent in alkali resistance, heat resistance and freezing resistance and good in anti-crack effect; according to actual determination of the inventor, the density of the civil building anti-crack mortar is only 1300-1500 kg/m < 3 >, and the civil building anti-crack mortar is light in weight and good in effect; according to the preparation method, the raw materials only need to be mixed and stirred, the process is simple and easy to control, and large-scale production is facilitated.
本发明涉及一种民用建筑抗裂砂浆及其制备方法。所述民用建筑抗裂砂浆,包括如下重量份的原料:硅酸盐水泥200~350份、机制砂400~500份、橡胶颗粒100~200份、复合掺合料50~80份、纤维素醚2~3份、可再分散乳胶粉5~15份、淀粉醚0.1~0.3份和聚丙烯纤维1~3份。所述民用建筑抗裂砂浆,将多种成分进行科学配合,使其具有良好的综合性能,其凝结时间短,强度高,耐碱、耐热、抗冻性优异,抗裂效果好;且经发明人实际测定,所述民用建筑抗裂砂浆密度仅为1300~1500kg/m3,质轻效果佳;所述制备方法,仅需将原料混合后搅拌即可,工艺简单、易控,有利于规模化产出。
Civil building anti-crack mortar and preparation method thereof
The invention relates to civil building anti-crack mortar and a preparation method thereof. The civil building anti-crack mortar is prepared from the following raw materials in parts by weight: 200 to 350 parts of Portland cement, 400 to 500 parts of machine-made sand, 100 to 200 parts of rubber particles, 50 to 80 parts of composite admixture, 2 to 3 parts of cellulose ether, 5 to 15 parts of redispersible latex powder, 0.1 to 0.3 part of starch ether and 1 to 3 parts of polypropylene fiber. According to the civil building anti-crack mortar, various components are scientifically matched, so that the civil building anti-crack mortar has good comprehensive performance and is short in setting time, high in strength, excellent in alkali resistance, heat resistance and freezing resistance and good in anti-crack effect; according to actual determination of the inventor, the density of the civil building anti-crack mortar is only 1300-1500 kg/m < 3 >, and the civil building anti-crack mortar is light in weight and good in effect; according to the preparation method, the raw materials only need to be mixed and stirred, the process is simple and easy to control, and large-scale production is facilitated.
本发明涉及一种民用建筑抗裂砂浆及其制备方法。所述民用建筑抗裂砂浆,包括如下重量份的原料:硅酸盐水泥200~350份、机制砂400~500份、橡胶颗粒100~200份、复合掺合料50~80份、纤维素醚2~3份、可再分散乳胶粉5~15份、淀粉醚0.1~0.3份和聚丙烯纤维1~3份。所述民用建筑抗裂砂浆,将多种成分进行科学配合,使其具有良好的综合性能,其凝结时间短,强度高,耐碱、耐热、抗冻性优异,抗裂效果好;且经发明人实际测定,所述民用建筑抗裂砂浆密度仅为1300~1500kg/m3,质轻效果佳;所述制备方法,仅需将原料混合后搅拌即可,工艺简单、易控,有利于规模化产出。
Civil building anti-crack mortar and preparation method thereof
一种民用建筑抗裂砂浆及其制备方法
PENG BO (author) / HU KAI (author) / LIU XIAOQIANG (author) / WANG YUAN (author) / YANG HUA (author)
2022-07-12
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2023
|Anti-crack plastering mortar and preparation method thereof
European Patent Office | 2023
|