Anti-crack mortar raw material for aerated building block and preparation method of anti-crack mortar
The invention discloses an anti-crack mortar raw material for aerated building blocks and a preparation method of anti-crack mortar, and relates to the technical field of aerated building blocks, the anti-crack mortar raw material comprises the following components by weight: 60-70 parts of fine sand, 10-15 parts of cement, 10-15 parts of lime, 10-15 parts of gypsum powder, 3-10 parts of grid fiber cloth, and 2-5 parts of a plant fiber mixture; 1-3 parts of a foaming agent, 3-10 parts of a stabilizing agent and 100-120 parts of water. The grid fibers are spirally arranged in the aerated building block mold in the aerated building block anti-crack mortar, the obtained aerated building block anti-crack mortar has high toughness and can be suitable for high-strength wall construction, plant fiber mixed materials are added into the aerated building block anti-crack mortar, and the aerated building block anti-crack mortar is formed. The plant fiber mixture is soaked in the mixed solution of zinc dichloride and phosphoric acid and absolute ethyl alcohol, the obtained plant fiber mixture is higher in toughness and purity, and the strength of the finished aerated building block can be greatly improved.
本发明公开了一种用于加气砌块的抗裂砂浆原料及抗裂砂浆的制备方法,涉及加气砌块技术领域,以重量份计,所述抗裂砂浆原料的配方包括:细砂:60份~70份,水泥:10份~15份,石灰:10份~15份,石膏粉:10份~15份,网格纤维布:3份~10份,植物纤维混料:2份~5份;发气剂:1份~3份,稳定剂:3份~10份,水:100份~120份。本发明通过在加气砌块抗裂砂浆中将网格纤维螺旋布置于加气砌块模具内部,得到的加气砌块抗裂砂浆具有较高韧性,可适用于高强度的墙体建造,在加气砌块抗裂砂浆中加入植物纤维混料,植物纤维混料经过二氯化锌与磷酸的混合液及无水乙醇浸泡,所得出的植物纤维混料韧性和纯度更高,能极大提高加气砌块成品强度。
Anti-crack mortar raw material for aerated building block and preparation method of anti-crack mortar
The invention discloses an anti-crack mortar raw material for aerated building blocks and a preparation method of anti-crack mortar, and relates to the technical field of aerated building blocks, the anti-crack mortar raw material comprises the following components by weight: 60-70 parts of fine sand, 10-15 parts of cement, 10-15 parts of lime, 10-15 parts of gypsum powder, 3-10 parts of grid fiber cloth, and 2-5 parts of a plant fiber mixture; 1-3 parts of a foaming agent, 3-10 parts of a stabilizing agent and 100-120 parts of water. The grid fibers are spirally arranged in the aerated building block mold in the aerated building block anti-crack mortar, the obtained aerated building block anti-crack mortar has high toughness and can be suitable for high-strength wall construction, plant fiber mixed materials are added into the aerated building block anti-crack mortar, and the aerated building block anti-crack mortar is formed. The plant fiber mixture is soaked in the mixed solution of zinc dichloride and phosphoric acid and absolute ethyl alcohol, the obtained plant fiber mixture is higher in toughness and purity, and the strength of the finished aerated building block can be greatly improved.
本发明公开了一种用于加气砌块的抗裂砂浆原料及抗裂砂浆的制备方法,涉及加气砌块技术领域,以重量份计,所述抗裂砂浆原料的配方包括:细砂:60份~70份,水泥:10份~15份,石灰:10份~15份,石膏粉:10份~15份,网格纤维布:3份~10份,植物纤维混料:2份~5份;发气剂:1份~3份,稳定剂:3份~10份,水:100份~120份。本发明通过在加气砌块抗裂砂浆中将网格纤维螺旋布置于加气砌块模具内部,得到的加气砌块抗裂砂浆具有较高韧性,可适用于高强度的墙体建造,在加气砌块抗裂砂浆中加入植物纤维混料,植物纤维混料经过二氯化锌与磷酸的混合液及无水乙醇浸泡,所得出的植物纤维混料韧性和纯度更高,能极大提高加气砌块成品强度。
Anti-crack mortar raw material for aerated building block and preparation method of anti-crack mortar
一种用于加气砌块的抗裂砂浆原料及抗裂砂浆的制备方法
LIN YUANBIAO (author) / SU SHUNFENG (author)
2023-05-16
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2021
|