A platform for research: civil engineering, architecture and urbanism
Decoration waste aerogel thermal insulation mortar and preparation method thereof
The invention relates to decoration waste aerogel thermal insulation mortar and a preparation method thereof. The decoration waste aerogel thermal insulation mortar is prepared from 102 parts of 52.5-grade cement, 630 to 900 parts of decoration waste recycled aggregate, 54 to 65 parts of aerogel, 11 parts of silica fume, 27.2 parts of slag, 68 parts of water, 1.1 parts of air entraining agent, 2.4 parts of water reducing agent and 0.9 part of polypropylene fiber. The thermal insulation mortar prepared according to the proportion has good mechanical property, excellent thermal insulation property and durability, and can greatly prolong the service life of an external thermal insulation material of an external wall when being applied to external thermal insulation engineering of the external wall in a frozen area.
一种装修垃圾气凝胶保温砂浆及其制备方法。所公开的装修垃圾气凝胶保温砂浆包括:52.5级水泥102份,装修垃圾再生骨料630~900份,气凝胶54~65份,硅灰11份,矿渣27.2份,水68份,引气剂1.1份,减水剂2.4份,聚丙烯纤维0.9份。本发明按配比制备的保温砂浆具有良好的力学性能,同时具备优异的保温性能与耐久性能,将其应用于受冻区外墙外保温工程中,可大幅提高外墙外保温材料的使用寿命。
Decoration waste aerogel thermal insulation mortar and preparation method thereof
The invention relates to decoration waste aerogel thermal insulation mortar and a preparation method thereof. The decoration waste aerogel thermal insulation mortar is prepared from 102 parts of 52.5-grade cement, 630 to 900 parts of decoration waste recycled aggregate, 54 to 65 parts of aerogel, 11 parts of silica fume, 27.2 parts of slag, 68 parts of water, 1.1 parts of air entraining agent, 2.4 parts of water reducing agent and 0.9 part of polypropylene fiber. The thermal insulation mortar prepared according to the proportion has good mechanical property, excellent thermal insulation property and durability, and can greatly prolong the service life of an external thermal insulation material of an external wall when being applied to external thermal insulation engineering of the external wall in a frozen area.
一种装修垃圾气凝胶保温砂浆及其制备方法。所公开的装修垃圾气凝胶保温砂浆包括:52.5级水泥102份,装修垃圾再生骨料630~900份,气凝胶54~65份,硅灰11份,矿渣27.2份,水68份,引气剂1.1份,减水剂2.4份,聚丙烯纤维0.9份。本发明按配比制备的保温砂浆具有良好的力学性能,同时具备优异的保温性能与耐久性能,将其应用于受冻区外墙外保温工程中,可大幅提高外墙外保温材料的使用寿命。
Decoration waste aerogel thermal insulation mortar and preparation method thereof
一种装修垃圾气凝胶保温砂浆及其制备方法
CHAE JIN WOO (author) / SU RUI (author) / GAO SHUAI (author) / REN ZIRONG (author) / ZHOU KAIJIN (author) / CHEN CHUNHONG (author) / ZHU PINGHUA (author) / LIU HUI (author) / ZHOU NIANYONG (author)
2023-06-09
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2024
|Aerogel modified thermal insulation mortar and preparation method thereof
European Patent Office | 2024
|European Patent Office | 2023
|Bi-component aerogel thermal insulation decorative mortar and preparation method thereof
European Patent Office | 2022
|Aerogel-glazed hollow bead thermal insulation mortar and preparation method thereof
European Patent Office | 2024
|