The invention particularly relates to a non-slip wear-resistant antibacterial ceramic tile and a preparation method thereof, the non-slip wear-resistant antibacterial ceramic tile sequentially comprises a green body layer, a cover glaze layer, a pattern texture layer, a non-slip wear-resistant layer and an antibacterial protective layer from bottom to top, and the antibacterial protective layer adopts nano zinc oxide and nano copper oxide which are compounded according to a certain proportion to serve as an antibacterial agent; the preparation method of the non-slip wear-resistant antibacterial ceramic tile comprises the following steps: preparing a green body, preparing cover glaze slurry, preparing non-slip wear-resistant slurry, preparing pattern textures, preparing antibacterial glaze slurry, and firing to obtain the non-slip wear-resistant antibacterial ceramic tile. The non-slip wear-resistant antibacterial ceramic tile has good antibacterial performance, and the antibacterial rate reaches 99% or above.
本发明具体涉及一种止滑耐磨抗菌瓷砖及其制备方法,该止滑耐磨抗菌瓷砖由下至上依次包括坯体层、面釉层、图案纹理层、止滑耐磨层和抗菌保护层,抗菌保护层采用纳米氧化锌和纳米氧化铜按一定的比例复合作为抗菌剂;该止滑耐磨抗菌瓷砖的制备方法包括步骤:坯体的制备,面釉浆料的制备,止滑耐磨浆料的制备,图案纹理的制备,抗菌釉浆的制备,烧制得止滑耐磨抗菌瓷砖。本发明的止滑耐磨抗菌瓷砖具有很好的抗细菌性能,抗菌率达到99%以上。
The invention particularly relates to a non-slip wear-resistant antibacterial ceramic tile and a preparation method thereof, the non-slip wear-resistant antibacterial ceramic tile sequentially comprises a green body layer, a cover glaze layer, a pattern texture layer, a non-slip wear-resistant layer and an antibacterial protective layer from bottom to top, and the antibacterial protective layer adopts nano zinc oxide and nano copper oxide which are compounded according to a certain proportion to serve as an antibacterial agent; the preparation method of the non-slip wear-resistant antibacterial ceramic tile comprises the following steps: preparing a green body, preparing cover glaze slurry, preparing non-slip wear-resistant slurry, preparing pattern textures, preparing antibacterial glaze slurry, and firing to obtain the non-slip wear-resistant antibacterial ceramic tile. The non-slip wear-resistant antibacterial ceramic tile has good antibacterial performance, and the antibacterial rate reaches 99% or above.
本发明具体涉及一种止滑耐磨抗菌瓷砖及其制备方法,该止滑耐磨抗菌瓷砖由下至上依次包括坯体层、面釉层、图案纹理层、止滑耐磨层和抗菌保护层,抗菌保护层采用纳米氧化锌和纳米氧化铜按一定的比例复合作为抗菌剂;该止滑耐磨抗菌瓷砖的制备方法包括步骤:坯体的制备,面釉浆料的制备,止滑耐磨浆料的制备,图案纹理的制备,抗菌釉浆的制备,烧制得止滑耐磨抗菌瓷砖。本发明的止滑耐磨抗菌瓷砖具有很好的抗细菌性能,抗菌率达到99%以上。
Anti-slip wear-resistant antibacterial ceramic tile and preparation method thereof
一种止滑耐磨抗菌瓷砖及其制备方法
YI SHIWEI (author)
2023-11-14
Patent
Electronic Resource
Chinese
Production process of antibacterial, wear-resistant and anti-slip glazed ceramic tile
European Patent Office | 2021
|Wear-resistant non-slip ceramic tile and preparation method thereof
European Patent Office | 2021
|Anti-slip super-wear-resistant ceramic tile and production process thereof
European Patent Office | 2024
|Anti-slip stain-resistant ceramic tile and preparation method thereof