A platform for research: civil engineering, architecture and urbanism
Green construction method for heat-preservation lightweight aggregate concrete floor
The invention relates to the technical field of floor construction, and discloses a heat-preservation lightweight aggregate concrete floor green construction method which comprises the following steps: S1, carrying out a series of treatment on a base layer of a concrete floor; s2, a leveling control line is bounced; s3, making a leveling elevation mud cake; s4, preparing a binding layer of lightweight aggregate concrete; s5, partition maintenance is carried out; a series of treatment specific implementation modes in the step S1 are as follows: S11, dust on a base layer of the concrete floor is treated by utilizing dust removal equipment; and S12, after dust removal is finished, the base layer of the concrete floor is cleaned through a handheld concrete bush hammer. The viscosity, corrosion resistance and crack resistance of the lightweight aggregate concrete can be enhanced by adding the silicon dioxide, the titanium dioxide powder, the anti-cracking agent and the calcium carbonate, the cohesiveness and hardness of the lightweight aggregate concrete can be enhanced by adding the modified glass beads, the water repellent and the ceramsite, and the overall performance of the lightweight aggregate concrete can be improved.
本发明涉及楼面施工技术领域,且公开了一种保温轻骨料混凝土楼面绿色施工方法,包括以下步骤:S1:将混凝土楼面的基层进行一系列处理;S2:弹找平控制线;S3:做找平面标高泥饼;S4:轻骨料混凝土的结合层;S5:隔档养护;S1步骤中的一系列处理具体实施方式为:S11:利用除尘设备对混凝土楼面的基层上的灰尘进行处理;S12:除尘结束后,利用手持式混凝土凿毛机对混凝土楼面的基层进行清理处理。本发明通过加入的二氧化硅、二氧化钛粉、抗裂剂、碳酸钙可以加强轻骨料混凝土的粘性、耐腐蚀性,以及抗裂性,通过加入的改性玻化微珠、憎水剂、陶粒可以加强轻骨料混凝土的粘结性以及硬度,可以改善强轻骨料混凝土的整体性能。
Green construction method for heat-preservation lightweight aggregate concrete floor
The invention relates to the technical field of floor construction, and discloses a heat-preservation lightweight aggregate concrete floor green construction method which comprises the following steps: S1, carrying out a series of treatment on a base layer of a concrete floor; s2, a leveling control line is bounced; s3, making a leveling elevation mud cake; s4, preparing a binding layer of lightweight aggregate concrete; s5, partition maintenance is carried out; a series of treatment specific implementation modes in the step S1 are as follows: S11, dust on a base layer of the concrete floor is treated by utilizing dust removal equipment; and S12, after dust removal is finished, the base layer of the concrete floor is cleaned through a handheld concrete bush hammer. The viscosity, corrosion resistance and crack resistance of the lightweight aggregate concrete can be enhanced by adding the silicon dioxide, the titanium dioxide powder, the anti-cracking agent and the calcium carbonate, the cohesiveness and hardness of the lightweight aggregate concrete can be enhanced by adding the modified glass beads, the water repellent and the ceramsite, and the overall performance of the lightweight aggregate concrete can be improved.
本发明涉及楼面施工技术领域,且公开了一种保温轻骨料混凝土楼面绿色施工方法,包括以下步骤:S1:将混凝土楼面的基层进行一系列处理;S2:弹找平控制线;S3:做找平面标高泥饼;S4:轻骨料混凝土的结合层;S5:隔档养护;S1步骤中的一系列处理具体实施方式为:S11:利用除尘设备对混凝土楼面的基层上的灰尘进行处理;S12:除尘结束后,利用手持式混凝土凿毛机对混凝土楼面的基层进行清理处理。本发明通过加入的二氧化硅、二氧化钛粉、抗裂剂、碳酸钙可以加强轻骨料混凝土的粘性、耐腐蚀性,以及抗裂性,通过加入的改性玻化微珠、憎水剂、陶粒可以加强轻骨料混凝土的粘结性以及硬度,可以改善强轻骨料混凝土的整体性能。
Green construction method for heat-preservation lightweight aggregate concrete floor
一种保温轻骨料混凝土楼面绿色施工方法
LIU YAN (author) / KANG LIEJUN (author) / XIE LUNYI (author) / DAI YIHUI (author) / ZOU JIANXIN (author)
2023-12-12
Patent
Electronic Resource
Chinese
Green construction method for heat-preservation lightweight aggregate concrete floor
European Patent Office | 2023
|Green construction method for heat-preservation lightweight aggregate concrete floor
European Patent Office | 2023
|Green lightweight aggregate concrete and building floor construction method
European Patent Office | 2022
|LIGHTWEIGHT CONCRETE FLOOR SLAB AND LIGHTWEIGHT CONCRETE FLOOR SLAB CONSTRUCTION METHOD
European Patent Office | 2023
|