Construction method of acid and alkali resistant industrial brick floor
The invention discloses a construction method of an acid and alkali resistant industrial brick floor. The construction method comprises the following steps: step 1) base layer treatment; 2) measuring a base layer; (3) paving a base layer; 4) processing a base layer parting line; (5) preparing before paving the ground; (6) paving by a tooth groove method; (7) gap pouring; according to the construction method of the acid and alkali resistant industrial brick floor, operation is easy, the floor prepared through the construction method has the advantages of being resistant to acid and alkali, high and low temperature and chemical corrosion, damage or holes, caused by acid, alkali and the like, of the floor can be effectively avoided, and the service life of floor bricks can be prolonged.
本发明公开了一种耐酸碱工业砖地面的施工方法,包括如下步骤:步骤1)基层处理;步骤2)基层测量;步骤3)基层摊铺;步骤4)基层分割线处理;步骤5)地面铺贴前准备;步骤6)齿沟法铺贴;步骤7)缝隙浇灌;本发明所述的耐酸碱工业砖地面的施工方法,操作简易,通过施工方法所制备而成的地面具有耐酸碱、耐高低温、耐化学腐蚀的优点,可有效规避地面因酸碱等造成的破损或孔洞,可延长地面砖的使用寿命。
Construction method of acid and alkali resistant industrial brick floor
The invention discloses a construction method of an acid and alkali resistant industrial brick floor. The construction method comprises the following steps: step 1) base layer treatment; 2) measuring a base layer; (3) paving a base layer; 4) processing a base layer parting line; (5) preparing before paving the ground; (6) paving by a tooth groove method; (7) gap pouring; according to the construction method of the acid and alkali resistant industrial brick floor, operation is easy, the floor prepared through the construction method has the advantages of being resistant to acid and alkali, high and low temperature and chemical corrosion, damage or holes, caused by acid, alkali and the like, of the floor can be effectively avoided, and the service life of floor bricks can be prolonged.
本发明公开了一种耐酸碱工业砖地面的施工方法,包括如下步骤:步骤1)基层处理;步骤2)基层测量;步骤3)基层摊铺;步骤4)基层分割线处理;步骤5)地面铺贴前准备;步骤6)齿沟法铺贴;步骤7)缝隙浇灌;本发明所述的耐酸碱工业砖地面的施工方法,操作简易,通过施工方法所制备而成的地面具有耐酸碱、耐高低温、耐化学腐蚀的优点,可有效规避地面因酸碱等造成的破损或孔洞,可延长地面砖的使用寿命。
Construction method of acid and alkali resistant industrial brick floor
一种耐酸碱工业砖地面的施工方法
DENG GUANGHUAN (author) / CUI JINZHAO (author) / CHEN BAOZHU (author) / LIU CHUNBO (author) / CHAI XIAOYING (author)
2023-12-22
Patent
Electronic Resource
Chinese
IPC:
E04F
FINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS
,
Ausbau von Bauwerken, z.B. Treppen, Fußböden
Novel acid-resistant alkali-resistant carbon brick and preparation method thereof
European Patent Office | 2021
|Preparation method of high-strength alkali-resistant brick
European Patent Office | 2020
|Novel self-releasing glaze fire-resistant alkali-resistant brick
European Patent Office | 2024
|European Patent Office | 2022
|