Two-component flexible ceramic tile adhesive material and preparation method thereof
The invention relates to a two-component flexible ceramic tile adhesive material and a preparation method thereof. The two-component flexible ceramic tile adhesive material comprises a liquid material component A and a liquid material component B, wherein the liquid material component A comprises 19-25% of styrene-butadiene emulsion, 0.05-0.13% of a defoaming agent, 0.05-0.13% of a sterilizing agent and 78-81% of water; the powder component B is prepared from 43 to 52 percent of cement, 47 to 51 percent of river sand, 2.5 to 4 percent of active filler, 0.3 to 0.5 percent of cellulose ether, 0.3 to 0.5 percent of sodium pyrophosphate and 0.2 to 0.4 percent of thixotropic agent; the weight ratio of the liquid material component to the powder material component is (26-30): 100; wherein the active filler is a combination of metakaolin and glass powder, and the ratio of metakaolin to glass powder is 2: 1. According to the bi-component flexible ceramic tile adhesive material and the preparation method thereof, the composition and proportion of the liquid component A and the powder component B are designed, and the flexibility of the ceramic tile adhesive is improved to absorb stress generated due to base material deformation, temperature difference and the like, so that the risk of falling of exterior wall ceramic tiles is reduced.
一种双组分柔性瓷砖胶材料及其制备方法,其包括液料组分A:丁苯乳液19~25%,消泡剂0.05~0.13%,杀菌剂0.05~0.13%,水78~81%;粉料组分B:水泥43~52%,河沙47~51%,活性填料2.5~4%,纤维素醚0.3~0.5%,焦磷酸钠0.3~0.5%,触变剂0.2~0.4%;液料组分和粉料组分的重量比为:26~30:100;其中所述活性填料为偏高岭土、玻璃粉的组合,偏高领土:玻璃粉=2:1。本发明的双组分柔性瓷砖胶材料及其制备方法,通过设计液料组分A和粉料组分B的组成及配比,通过提高瓷砖胶柔韧性来吸收由于基材形变、温差等原因产生的应力,从而降低外墙瓷砖掉砖风险。
Two-component flexible ceramic tile adhesive material and preparation method thereof
The invention relates to a two-component flexible ceramic tile adhesive material and a preparation method thereof. The two-component flexible ceramic tile adhesive material comprises a liquid material component A and a liquid material component B, wherein the liquid material component A comprises 19-25% of styrene-butadiene emulsion, 0.05-0.13% of a defoaming agent, 0.05-0.13% of a sterilizing agent and 78-81% of water; the powder component B is prepared from 43 to 52 percent of cement, 47 to 51 percent of river sand, 2.5 to 4 percent of active filler, 0.3 to 0.5 percent of cellulose ether, 0.3 to 0.5 percent of sodium pyrophosphate and 0.2 to 0.4 percent of thixotropic agent; the weight ratio of the liquid material component to the powder material component is (26-30): 100; wherein the active filler is a combination of metakaolin and glass powder, and the ratio of metakaolin to glass powder is 2: 1. According to the bi-component flexible ceramic tile adhesive material and the preparation method thereof, the composition and proportion of the liquid component A and the powder component B are designed, and the flexibility of the ceramic tile adhesive is improved to absorb stress generated due to base material deformation, temperature difference and the like, so that the risk of falling of exterior wall ceramic tiles is reduced.
一种双组分柔性瓷砖胶材料及其制备方法,其包括液料组分A:丁苯乳液19~25%,消泡剂0.05~0.13%,杀菌剂0.05~0.13%,水78~81%;粉料组分B:水泥43~52%,河沙47~51%,活性填料2.5~4%,纤维素醚0.3~0.5%,焦磷酸钠0.3~0.5%,触变剂0.2~0.4%;液料组分和粉料组分的重量比为:26~30:100;其中所述活性填料为偏高岭土、玻璃粉的组合,偏高领土:玻璃粉=2:1。本发明的双组分柔性瓷砖胶材料及其制备方法,通过设计液料组分A和粉料组分B的组成及配比,通过提高瓷砖胶柔韧性来吸收由于基材形变、温差等原因产生的应力,从而降低外墙瓷砖掉砖风险。
Two-component flexible ceramic tile adhesive material and preparation method thereof
双组分柔性瓷砖胶材料及其制备方法
PANG JIAQI (author) / CHEN ZHENGZHONG (author) / CAO CHUN (author) / WU YONGWEN (author)
2024-04-26
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Two-component ceramic tile back adhesive and preparation method thereof
European Patent Office | 2023
|Two-component ceramic tile back adhesive and preparation method thereof
European Patent Office | 2022
|Two-component ceramic tile adhesive and preparation process thereof
European Patent Office | 2023
|