The low-energy-consumption high-strength high-toughness soft porcelain comprises a bottom layer, a middle layer and a surface layer which are sequentially arranged from bottom to top, the bottom layer is obtained by curing bottom layer slurry, the middle layer is a glass fiber net, and the surface layer is obtained by curing surface layer slurry; the bottom layer slurry is prepared from the following components in parts by mass: 3 to 5 parts of cement, 8 to 10 parts of emulsion, 45 to 53 parts of quartz sand, 12 to 20 parts of silicon carbide, 20 to 22 parts of calcium powder, 10 to 15 parts of water and 8 to 10 parts of water reducing agent; the surface layer slurry is prepared from the following components in parts by mass: 3 to 5 parts of cement, 8 to 10 parts of emulsion, 55 to 60 parts of quartz sand, 5 to 10 parts of silicon carbide, 6 to 12 parts of metal microfiber, 20 to 22 parts of calcium powder, 10 to 15 parts of water and 8 to 10 parts of water reducing agent. The low-energy-consumption, high-strength and high-toughness soft porcelain provided by the invention has relatively high toughness and strength, so that the soft porcelain can simultaneously consider low energy consumption, high strength and high flexibility to overcome the defects in the prior art.
本发明公开了一种低能耗高强度高韧性软瓷,包括由下至上依次设置的底层、中间层和面层;底层由底层浆料固化得到,中间层为玻璃纤维网,面层由面层浆料固化得到;按照质量份数计算,底层浆料包括水泥3~5份、乳液8~10份、石英砂45~53份、碳化硅12~20份、钙粉20~22份、水10~15份和减水剂8~10份;按照质量份数计算,面层浆料包括水泥3~5份、乳液8~10份、石英砂55~60份、碳化硅5~10份、金属微纤维6~12份、钙粉20~22份、水10~15份和减水剂8~10份。本发明提出的一种低能耗高强度高韧性软瓷,其具有较高的韧性和强度,使得软瓷可同时兼顾低能耗、高强度和高柔韧性,以克服现有技术的不足。
Low-energy-consumption high-strength high-toughness soft porcelain and preparation method thereof
The low-energy-consumption high-strength high-toughness soft porcelain comprises a bottom layer, a middle layer and a surface layer which are sequentially arranged from bottom to top, the bottom layer is obtained by curing bottom layer slurry, the middle layer is a glass fiber net, and the surface layer is obtained by curing surface layer slurry; the bottom layer slurry is prepared from the following components in parts by mass: 3 to 5 parts of cement, 8 to 10 parts of emulsion, 45 to 53 parts of quartz sand, 12 to 20 parts of silicon carbide, 20 to 22 parts of calcium powder, 10 to 15 parts of water and 8 to 10 parts of water reducing agent; the surface layer slurry is prepared from the following components in parts by mass: 3 to 5 parts of cement, 8 to 10 parts of emulsion, 55 to 60 parts of quartz sand, 5 to 10 parts of silicon carbide, 6 to 12 parts of metal microfiber, 20 to 22 parts of calcium powder, 10 to 15 parts of water and 8 to 10 parts of water reducing agent. The low-energy-consumption, high-strength and high-toughness soft porcelain provided by the invention has relatively high toughness and strength, so that the soft porcelain can simultaneously consider low energy consumption, high strength and high flexibility to overcome the defects in the prior art.
本发明公开了一种低能耗高强度高韧性软瓷,包括由下至上依次设置的底层、中间层和面层;底层由底层浆料固化得到,中间层为玻璃纤维网,面层由面层浆料固化得到;按照质量份数计算,底层浆料包括水泥3~5份、乳液8~10份、石英砂45~53份、碳化硅12~20份、钙粉20~22份、水10~15份和减水剂8~10份;按照质量份数计算,面层浆料包括水泥3~5份、乳液8~10份、石英砂55~60份、碳化硅5~10份、金属微纤维6~12份、钙粉20~22份、水10~15份和减水剂8~10份。本发明提出的一种低能耗高强度高韧性软瓷,其具有较高的韧性和强度,使得软瓷可同时兼顾低能耗、高强度和高柔韧性,以克服现有技术的不足。
Low-energy-consumption high-strength high-toughness soft porcelain and preparation method thereof
一种低能耗高强度高韧性软瓷及其制备方法
WANG XIAOJIAO (author) / CHEN ZHIFENG (author) / PAN HUANHUAN (author) / ZHANG ZHIWEN (author) / LI ZHIHONG (author)
2024-11-15
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
High-toughness white porcelain and preparation method thereof
European Patent Office | 2021
|European Patent Office | 2021
|High-toughness conical suspension type porcelain insulator and preparation method thereof
European Patent Office | 2021
|High-toughness conical suspension type porcelain insulator and preparation method thereof
European Patent Office | 2022
|High-strength porcelain biscuit and preparation method thereof
European Patent Office | 2021
|