A platform for research: civil engineering, architecture and urbanism
Recycled asphalt mixture and preparation device thereof
The invention relates to a recycled asphalt mixture and a preparation device thereof, the recycled asphalt mixture comprises the following components in parts by mass: 100-120 parts of waste asphalt mixture, 20-30 parts of aggregate, 18-24 parts of mineral admixture, 0.8-1 part of fiber, 8-15 parts of asphalt regenerant and 3-5 parts of new asphalt, and the recycled asphalt mixture is prepared from the following components in parts by mass: 100-120 parts of waste asphalt mixture, 20-30 parts of aggregate, 18-24 parts of mineral admixture, 0.8-1 part of fiber, 8-15 parts of asphalt regenerant and 3-5 parts of new asphalt. The method further comprises the following preparation steps that the aged asphalt pavement is milled, a waste asphalt mixture is obtained, the waste asphalt mixture, the aggregate, the mineral admixture and the new asphalt are preheated and subjected to heat preservation, and the preheated waste asphalt mixture and the asphalt recycling agent are added into a recycled asphalt mixture preparation device to be stirred and mixed; adding the preheated aggregate, stirring and mixing, sequentially adding the mineral admixture, the fiber and the new asphalt, and stirring and mixing to obtain the recycled asphalt mixture.
本发明涉及一种再生沥青混合料及其制备装置,包括废旧沥青混合料、骨料、矿物掺合料、纤维、沥青再生剂以及新沥青,按质量份数由以下组分组成,其中废旧沥青混合料100‑120份,骨料20‑30份,矿物掺合料18‑24份,纤维0.8‑1份,沥青再生剂8‑15份,新沥青3‑5份,还包括以下制备步骤,对老化后的沥青路面进行铣刨,获得废旧沥青混合料,将废旧沥青混合料、骨料、矿物掺合料和新沥青预热并保温,将预热后的废旧沥青混合料与沥青再生剂添加至再生沥青混合料制备装置中进行搅拌混合;然后在添加预热后的骨料进行搅拌混合,再依次添加矿物掺合料、纤维和新沥青进行搅拌混合获得再生沥青混合料。
Recycled asphalt mixture and preparation device thereof
The invention relates to a recycled asphalt mixture and a preparation device thereof, the recycled asphalt mixture comprises the following components in parts by mass: 100-120 parts of waste asphalt mixture, 20-30 parts of aggregate, 18-24 parts of mineral admixture, 0.8-1 part of fiber, 8-15 parts of asphalt regenerant and 3-5 parts of new asphalt, and the recycled asphalt mixture is prepared from the following components in parts by mass: 100-120 parts of waste asphalt mixture, 20-30 parts of aggregate, 18-24 parts of mineral admixture, 0.8-1 part of fiber, 8-15 parts of asphalt regenerant and 3-5 parts of new asphalt. The method further comprises the following preparation steps that the aged asphalt pavement is milled, a waste asphalt mixture is obtained, the waste asphalt mixture, the aggregate, the mineral admixture and the new asphalt are preheated and subjected to heat preservation, and the preheated waste asphalt mixture and the asphalt recycling agent are added into a recycled asphalt mixture preparation device to be stirred and mixed; adding the preheated aggregate, stirring and mixing, sequentially adding the mineral admixture, the fiber and the new asphalt, and stirring and mixing to obtain the recycled asphalt mixture.
本发明涉及一种再生沥青混合料及其制备装置,包括废旧沥青混合料、骨料、矿物掺合料、纤维、沥青再生剂以及新沥青,按质量份数由以下组分组成,其中废旧沥青混合料100‑120份,骨料20‑30份,矿物掺合料18‑24份,纤维0.8‑1份,沥青再生剂8‑15份,新沥青3‑5份,还包括以下制备步骤,对老化后的沥青路面进行铣刨,获得废旧沥青混合料,将废旧沥青混合料、骨料、矿物掺合料和新沥青预热并保温,将预热后的废旧沥青混合料与沥青再生剂添加至再生沥青混合料制备装置中进行搅拌混合;然后在添加预热后的骨料进行搅拌混合,再依次添加矿物掺合料、纤维和新沥青进行搅拌混合获得再生沥青混合料。
Recycled asphalt mixture and preparation device thereof
一种再生沥青混合料及其制备装置
LUO XIU (author) / ZHANG ZHIJUN (author) / YI ZHOUXIN (author) / LIN JUN (author)
2024-12-06
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
/
B01F
MIXING, e.g. DISSOLVING, EMULSIFYING, DISPERSING
,
Mischen, z.B. Lösen, Emulgieren, Dispergieren
/
B08B
Reinigen allgemein
,
CLEANING IN GENERAL
/
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
RECYCLED ASPHALT MIXTURE PRODUCTION METHOD AND RECYCLED ASPHALT MIXTURE PRODUCTION DEVICE
European Patent Office | 2021
|