A platform for research: civil engineering, architecture and urbanism
RARE-EARTH OXIDE BASED MONOLITHIC CHAMBER MATERIAL
PROBLEM TO BE SOLVED: To provide a solid sintered ceramic article with excellent plasma resistance.SOLUTION: A solid sintered ceramic article may include a solid solution comprising YOat a concentration of approximately 30 mol% to approximately 60 mol%, ErOat a concentration of approximately 20 mol% to approximately 60 mol%, and at least one of ZrO, GdO, and SiOat a concentration of approximately 0 mol% to approximately 30 mol%. Alternatively, the solid sintered ceramic article includes a solid solution comprising 40-100 mol% of YO, 0-50 mol% of ZrO, and 0-40 mol% of AlO.SELECTED DRAWING: Figure 2
【課題】耐プラズマ性に優れた固体焼結セラミックス物品を提供する。【解決手段】固体焼結セラミックス物品は、約30モル%〜約60モル%の濃度のY2O3と、約20モル%〜約60モル%の濃度のEr2O3と、約0モル%〜約30モル%の濃度のZrO2、Gd2O3、又はSiO2のうちの少なくとも1つとを含む固溶体を含むことができる。あるいはまた、固体焼結セラミックス物品は、40〜100モル%のY2O3と、0〜50モル%のZrO2と、0〜40モル%のAl2O3とを含む固溶体を含む。【選択図】図2
RARE-EARTH OXIDE BASED MONOLITHIC CHAMBER MATERIAL
PROBLEM TO BE SOLVED: To provide a solid sintered ceramic article with excellent plasma resistance.SOLUTION: A solid sintered ceramic article may include a solid solution comprising YOat a concentration of approximately 30 mol% to approximately 60 mol%, ErOat a concentration of approximately 20 mol% to approximately 60 mol%, and at least one of ZrO, GdO, and SiOat a concentration of approximately 0 mol% to approximately 30 mol%. Alternatively, the solid sintered ceramic article includes a solid solution comprising 40-100 mol% of YO, 0-50 mol% of ZrO, and 0-40 mol% of AlO.SELECTED DRAWING: Figure 2
【課題】耐プラズマ性に優れた固体焼結セラミックス物品を提供する。【解決手段】固体焼結セラミックス物品は、約30モル%〜約60モル%の濃度のY2O3と、約20モル%〜約60モル%の濃度のEr2O3と、約0モル%〜約30モル%の濃度のZrO2、Gd2O3、又はSiO2のうちの少なくとも1つとを含む固溶体を含むことができる。あるいはまた、固体焼結セラミックス物品は、40〜100モル%のY2O3と、0〜50モル%のZrO2と、0〜40モル%のAl2O3とを含む固溶体を含む。【選択図】図2
RARE-EARTH OXIDE BASED MONOLITHIC CHAMBER MATERIAL
希土類酸化物系モノリシックチャンバ材料
JENNIFER Y SUN (author) / BIRAJA P KANUNGO (author)
2018-03-29
Patent
Electronic Resource
Japanese