SEMI-IMMERSION NOZZLE
PROBLEM TO BE SOLVED: To provide a semi-immersion nozzle excellent in tolerance in the vicinity of a meniscus at the inside of the nozzle and at the powder line part on the outside of the nozzle.SOLUTION: A semi-immersion nozzle is provided with: an inside member 2 arranged at the inside of a nozzle 1; and an outside member 3 arranged at the outside of the nozzle 1. The inside member 2 is composed of a spinel-carbon-silicon carbide material including: a spinel raw material of 75 to 95 mass%; a carbon raw material of 5 to 25 mass%; and silicon carbon of 1 to 8 mass% in outer percentage to the whole quantity of the spinel raw material and the carbon raw material. The outside member 3 is composed of a zirconia-carbon material including: a zirconia raw material of 50 to 90 mass%; and a carbon raw material of 10 to 50 mass%.SELECTED DRAWING: Figure 3
【課題】ノズル内側のメニスカス付近およびノズル外側のパウダーライン部での耐用性に優れたセミイマージョンノズルを提供する。【解決手段】ノズル1の内側に配置される内側部材2とノズル1の外側に配置される外側部材3とを備える。内側部材2は、スピネル原料75〜95質量%と、カーボン原料5〜25質量%と、スピネル原料とカーボン原料とカーボン原料との全量に対して外掛け1〜8質量%の炭化珪素質とを含有するスピネル−カーボン−炭化珪素質材質により構成される。外側部材3は、ジルコニア原料50〜90質量%と、カーボン原料10〜50質量%とを含有するジルコニア−カーボン質材質により構成される。【選択図】図3
SEMI-IMMERSION NOZZLE
PROBLEM TO BE SOLVED: To provide a semi-immersion nozzle excellent in tolerance in the vicinity of a meniscus at the inside of the nozzle and at the powder line part on the outside of the nozzle.SOLUTION: A semi-immersion nozzle is provided with: an inside member 2 arranged at the inside of a nozzle 1; and an outside member 3 arranged at the outside of the nozzle 1. The inside member 2 is composed of a spinel-carbon-silicon carbide material including: a spinel raw material of 75 to 95 mass%; a carbon raw material of 5 to 25 mass%; and silicon carbon of 1 to 8 mass% in outer percentage to the whole quantity of the spinel raw material and the carbon raw material. The outside member 3 is composed of a zirconia-carbon material including: a zirconia raw material of 50 to 90 mass%; and a carbon raw material of 10 to 50 mass%.SELECTED DRAWING: Figure 3
【課題】ノズル内側のメニスカス付近およびノズル外側のパウダーライン部での耐用性に優れたセミイマージョンノズルを提供する。【解決手段】ノズル1の内側に配置される内側部材2とノズル1の外側に配置される外側部材3とを備える。内側部材2は、スピネル原料75〜95質量%と、カーボン原料5〜25質量%と、スピネル原料とカーボン原料とカーボン原料との全量に対して外掛け1〜8質量%の炭化珪素質とを含有するスピネル−カーボン−炭化珪素質材質により構成される。外側部材3は、ジルコニア原料50〜90質量%と、カーボン原料10〜50質量%とを含有するジルコニア−カーボン質材質により構成される。【選択図】図3
SEMI-IMMERSION NOZZLE
セミイマージョンノズル
OGATA KAZUNOBU (author) / NISHIO KANAE (author) / NIIZUMA HIROYASU (author)
2018-05-17
Patent
Electronic Resource
Japanese
Immersion construction system and immersion construction method of semi-suspension type cofferdam
European Patent Office | 2024
|Taylor & Francis Verlag | 2019
|European Patent Office | 2023
|