METHOD FOR SUPPRESSING ELUTION OF BORON IN BORON-INCLUDING MATERIAL, AND METHOD FOR PRODUCTION OF TREATMENT MATERIAL FOR BORON ELUTION SUPPRESSION
To suppress the elution of boron in a boron-including material by a simple and easy method.SOLUTION: There is provided a boron elution-suppressing method suppressing the elution of boron from a boron-including material. The method is characterized by satisfying the expression (1): Z≥A×B(here, the cooling speeds Z and A express the time ratios of temperature change when cooling the boron-including material from the temperature of the boron-including material having a liquid phase to 900°C) when defining a cooling speed (unit: °C/min) in cooldown of the boron-including material in a temperature state having the liquid phase as Z, the cooling speed (unit: °C/min) in a range from 0.1°C/min to 20°C/min as A and the boron elution amount (unit: mg/L) of the boron-including material after cooling in the cooling speed A as B.SELECTED DRAWING: None
【課題】簡便な手法により、ホウ素含有物質のホウ素溶出を抑制する。【解決手段】ホウ素含有物質からホウ素が溶出することを抑制する、ホウ素含有物質のホウ素溶出抑制方法であって、液相を有する温度状態にある上記ホウ素含有物質を冷却し、上記ホウ素含有物質を冷却するときの冷却速度(単位:℃/min)をZ、0.1℃/min以上20℃/min以下の範囲の冷却速度(単位:℃/min)をA、上記冷却速度Aで冷却した後の上記ホウ素含有物質のホウ素溶出量(単位:mg/L)をBとしたときに、下記式(1)を満たす、ホウ素含有物質のホウ素溶出抑制方法。Z≧A×B3・・・(1)ただし、上記冷却速度ZおよびAは、上記ホウ素含有物質を、液相を有する温度から900℃まで冷却する際の温度変化の時間割合を表す。【選択図】なし
METHOD FOR SUPPRESSING ELUTION OF BORON IN BORON-INCLUDING MATERIAL, AND METHOD FOR PRODUCTION OF TREATMENT MATERIAL FOR BORON ELUTION SUPPRESSION
To suppress the elution of boron in a boron-including material by a simple and easy method.SOLUTION: There is provided a boron elution-suppressing method suppressing the elution of boron from a boron-including material. The method is characterized by satisfying the expression (1): Z≥A×B(here, the cooling speeds Z and A express the time ratios of temperature change when cooling the boron-including material from the temperature of the boron-including material having a liquid phase to 900°C) when defining a cooling speed (unit: °C/min) in cooldown of the boron-including material in a temperature state having the liquid phase as Z, the cooling speed (unit: °C/min) in a range from 0.1°C/min to 20°C/min as A and the boron elution amount (unit: mg/L) of the boron-including material after cooling in the cooling speed A as B.SELECTED DRAWING: None
【課題】簡便な手法により、ホウ素含有物質のホウ素溶出を抑制する。【解決手段】ホウ素含有物質からホウ素が溶出することを抑制する、ホウ素含有物質のホウ素溶出抑制方法であって、液相を有する温度状態にある上記ホウ素含有物質を冷却し、上記ホウ素含有物質を冷却するときの冷却速度(単位:℃/min)をZ、0.1℃/min以上20℃/min以下の範囲の冷却速度(単位:℃/min)をA、上記冷却速度Aで冷却した後の上記ホウ素含有物質のホウ素溶出量(単位:mg/L)をBとしたときに、下記式(1)を満たす、ホウ素含有物質のホウ素溶出抑制方法。Z≧A×B3・・・(1)ただし、上記冷却速度ZおよびAは、上記ホウ素含有物質を、液相を有する温度から900℃まで冷却する際の温度変化の時間割合を表す。【選択図】なし
METHOD FOR SUPPRESSING ELUTION OF BORON IN BORON-INCLUDING MATERIAL, AND METHOD FOR PRODUCTION OF TREATMENT MATERIAL FOR BORON ELUTION SUPPRESSION
ホウ素含有物質のホウ素溶出抑制方法、および、ホウ素溶出抑制処理材の製造方法
INOUE YOTARO (author) / FUJII YUSUKE (author) / YAMADA KATSUMI (author) / MATSUNAGA HISAHIRO (author) / WATANABE KEIJI (author)
2020-03-05
Patent
Electronic Resource
Japanese
European Patent Office | 2020
|METHOD FOR SUPPRESSING HEXAVALENT CHROMIUM ELUTION FROM SLAG
European Patent Office | 2016
|European Patent Office | 2021
|European Patent Office | 2021
|